Effect of Melt-Mixing Duration on the Thermal Degradation and Apparent Activation Energy of Low-Loading PS/NiFe2O4 Nanocomposites: A Sensitivity-Assessed Kinetic Analysis.
Aytekin Ulutaş
Edremit School of Civil Aviation, Balıkesir University, 10300 Edremit, Balıkesir, Türkiye.
Key points
From the paper's conclusion- PS/NiFe2O4 nanocomposites containing 2.5 wt.% NiFe2O4 were melt-blended in a twin-screw micro-compounder for 6 and 12 min (PS-NF-6 and PS-NF-12) and compared with neat PS processed for 6 min to examine whether mixing duration at a fixed low loading affects thermal degradation and apparent kinetics.
Abstract
PS/NiFe2O4 nanocomposites containing 2.5 wt.% NiFe2O4 were melt-blended in a twin-screw micro-compounder for 6 and 12 min (PS-NF-6 and PS-NF-12) and compared with neat PS processed for 6 min to examine whether mixing duration at a fixed low loading affects thermal degradation and apparent kinetics. XRD confirmed that the NiFe2O4 spinel structure was retained; surface SEM observations were treated as preliminary. TG data were normalized to the principal degradation step to minimize low-temperature mass-loss and balance-drift effects. PS-NF-12 degraded at higher temperatures than neat PS at all heating rates (5-20 K min-1), with mean shifts of 5-8 K over α = 0.05-0.80, whereas the effect of PS-NF-6 was limited to the early stage. Kissinger apparent activation energies (Ea) were 194 ± 18, 201 ± 14, and 252 ± 12 kJ mol-1 for PS, PS-NF-6, and PS-NF-12, respectively, and PS-NF-12 remained the highest when any single heating rate was omitted. The KAS conversion-dependent activation energy (Eα) of PS-NF-12 increased with conversion only when the 5 K min-1 run was included; without it, Eα remained at 206-212 kJ mol-1. At constant low loading, longer mixing was thus associated with delayed mass loss and a higher peak-region Ea.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Dispersion-Controlled Thermal Degradation Kinetics of PMMA/NiFe₂O₄ Nanocomposites Prepared with Different Mixing TimesGazi Üniversitesi Fen Bilimleri Dergisi Part C Tasarım ve Teknoloji · 2026
- The Governing Role of Polymer Matrix in Tailoring the Functional Properties of Magnetite‐Filled NanocompositesPolymer Engineering and Science · 2026
- Structural, microstructure, magnetic, and dielectric characterization of BaFe12O19/NiFe2O4ferrite nanocompositesJournal of Sol-Gel Science and Technology · 2026
- Dielectric, Magnetic, and Thermal Studies of (1− x ) Ni 0.8 Mn 0.2 Fe 2 O 4 + x BaFeO 3 ( x = 0.2–0.8) NanocompositesChemistrySelect · 2026
- Thermal stability and degradation kinetics of PVC/PEO nanocomposites incorporating CoFe2O4 nanoparticlesJournal of Materials Science · 2026
- Interphase‐controlled crystallization and Maxwell–Wagner–Sillars polarization in hybrid polyether ether ketone–carbon fibre–TiB 2 compositesPolymer International · 2026