Ionic-Liquid-Catalyzed Depolymerization of PET: BHET Recovery and Re-Polymerization.
Akmuhammet Karayev, Farrukh Shehzad, Hassam Mazhar, Mamdouh A Al-Harthi
Department of Chemical Engineering, King Fahd University of Petroleum and Minerals, Dhahran 31261, Saudi Arabia. · Institute of Zhejiang University-Quzhou, Quzhou 324000, China.
Key points
From the paper's conclusion- The recovered BHET was characterized by FT-IR, 1H and 13C NMR and GC-MS, and further, was re-polymerized by melt polycondensation at 270 °C.
Abstract
The accumulation of polyethylene terephthalate (PET) waste presents significant environmental challenges due to its extensive usage and low global recycling rates. Among the available recycling routes, chemical depolymerization by glycolysis offers a promising way to recover high-value monomers. In this study, six ionic liquids (ILs) were tested as homogeneous catalysts for the glycolysis of post-consumer PET bottles in ethylene glycol (EG) at 200 °C for 3 h, alongside an uncatalyzed control. 1-Butyl-3-methylimidazolium acetate ([BMIM][OAc]) and trihexyltetradecylphosphonium decanoate ([P6,6,6,14][Dec]) gave complete PET conversion with isolated bis(2-hydroxyethyl) terephthalate (BHET) yields of 33.6% and 72.4%, respectively. Moreover, trihexyltetradecylphosphonium bis(2,4,4-trimethylpentyl)phosphinate ([P6,6,6,14][TMPP]) reached 56% conversion with no separable product; however, the other three chloride-based ILs and the control reaction demonstrated negligible conversion at the given process parameters. The recovered BHET was characterized by FT-IR, 1H and 13C NMR and GC-MS, and further, was re-polymerized by melt polycondensation at 270 °C. The FT-IR fingerprint, thermogravimetric decomposition profile and solid-state 13C NMR spectrum indicated that the properties of the recycled PET compete with those of the bottlegrade PET. Their melting peak lay 7.7 °C below the reference on first heating (240.6 vs. 248.3 °C) but rose to 248.5 °C on second heating, 3.3 °C above the reference, suggesting that the initial difference arises mainly from crystal perfection and thermal history rather than from an altered chain structure.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Imidazolium‐Based Ionic Liquids for PET Glycolysis: A Sustainable Approach for Plastic WastePolymer Engineering & Science · 2026
- Hydrolysis of 1,4-Butanediol-Derived Polyesters Into Tetrahydrofuran and Dicarboxylic Acids Over Lewis Acidic Ionic Liquids.ChemSusChem · 2026
- Metal Octoates as Lewis Acid Catalysts for the Hydrolytic Depolymerization of PET in TetrahydrofuranCatalysts · 2026
- Noncovalent Interaction-Catalyzed High Conversion of Waste PET Plastics into Organic Esters under Mild Conditions.Organic letters · 2026
- Robust cellular transformations of PET deconstruction products by import of glycol esters.Science advances · 2026
- Efficient Glycolysis of Waste PET at Room Temperature Enabled by a Bifunctional Catalyst System and Co-solventACS Sustainable Resource Management · 2026