Fabrication and Characterization of Polylactic Acid/Hyaluronic Acid/Collagen Nanofibers for Tendon Tissue Engineering.
Zekiye Akdag, Cengiz Kazdal, Elif Nur Yildiz, Zehra Kanli, Ridvan Yildirim, Ali Sahin, Fatih Eren, Oguzhan Gunduz
Department of Metallurgical and Materials Engineering, Graduate School of Science and Engineering, Marmara University, Istanbul 34854, Turkey. · Department of Orthopaedics and Traumatology, Faculty of Medicine, Recep Tayyip Erdogan University, Rize 53200, Turkey.
Key points
From the paper's conclusion- In human mesenchymal stem cells, viability was maintained or increased over 7 days on the coaxial scaffolds but declined markedly on the blend scaffolds, indicating that the core–shell architecture is more favorable for tendon tissue regeneration.
Abstract
Tendons are highly elastic connective tissues that transfer mechanical loads from muscle to bone, and their healing is often slow and incomplete because of limited vascularization. Tissue engineering approaches are therefore emerging as promising alternatives to support tendon repair. In this study, polylactic acid (PLA)-based nanofibers containing hyaluronic acid (HA) and collagen (COL), intrinsic components of the extracellular matrix, were fabricated by blend and coaxial electrospinning. Matrices of identical overall composition were produced by both configurations, so that the contribution of nanofiber architecture could be isolated from that of chemical composition; the coaxial nanofibers comprised a load-bearing PLA/COL core and a PLA/HA shell, reproducing the collagen-rich tendon proper and the hyaluronic acid-rich gliding surface of native tendon. Mean fiber diameters ranged from 319 ± 82 nm for neat PLA to 854 ± 220 nm for the coaxial nanofibers, approximately twice that of the compositionally identical blend nanofibers (454 ± 110 nm). Tensile strength increased from 2.108 MPa for neat PLA to 4.94 MPa for PLA/COL, and the coaxial nanofibers retained a comparable value (4.651 MPa, p > 0.05) despite the incorporation of HA. In human mesenchymal stem cells, viability was maintained or increased over 7 days on the coaxial scaffolds but declined markedly on the blend scaffolds, indicating that the core-shell architecture is more favorable for tendon tissue regeneration.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- An aligned-to-random PLA/PCL/COL1 bilayer electrospun scaffold loaded with exosomes of bone marrow-derived mesenchymal stem cells promotes tendon-to-bone healing in rats.Biomaterials advances · 2026
- Biomimetic Core–Sheath GelMA/PCL Nanofibers for Enhanced Peripheral Nerve RegenerationPolymers · 2026
- Dynamic Culture of TDSCs on a Mechanically Biomimetic PCL/COL Flexible SubstrateFlexTech · 2026
- Synergistic Reinforcing Effect of Stereo‐Complex Polylactide (Sc‐ PLA ) Staple Fiber and Hydroxyapatite ( HA ) on the Tensile Properties of PLA / HA /Sc‐ PLA Staple Fiber CompositesPolymer Composites · 2026
- Versatile twin layer macromolecular fibers for advanced tissue engineering applications.iScience · 2026
- Development and Characterization of a Dual Nanofibrillar Membrane of Polylactic Acid Loaded with Hydroxyapatite and Chlorhexidine for Guided Bone Regeneration.Polymers · 2026