Composition-Structure-Property Relationships in PLA-nHA-Mg Hybrid Biocomposites: Effect of Ceramic-Metallic Reinforcement Ratio on Mechanical and Physicochemical Performance.
K Hariharan, B Veera Siva Reddy, Dola Sundeep, C Chandrasekhara Sastry, Robert Cep
Department of Mechanical Engineering, Dr Mahalingam College of Engineering and Technology, Coimbatore 642003, Tamil Nadu, India. · Department of Mechanical Engineering, Indian Institute of Information Technology Design and Manufacturing Kurnool (IIITDM Kurnool), Kurnool 518008, Andhra Pradesh, India.
Key points
From the paper's conclusion- The results indicate that Mg:nHA partitioning alters the recorded loading-mode response within the tested 10 wt.% reinforcement window, while particle-scale mechanisms and biological performance require further validation.
Abstract
Poly(lactic acid) (PLA) hybridized with nano-hydroxyapatite (nHA) and elemental magnesium (Mg) offers a route to tune load-bearing behavior while retaining a biodegradable polymer matrix. This study compares neat PLA, binary PLA-10Mg and PLA-10nHA controls, and three ternary hybrids containing a constant 10 wt.% total reinforcement at Mg:nHA ratios of 1:1, 3:1, and 1:3. Tensile, compressive, and three-point flexural responses were interpreted together with differential scanning calorimetry (DSC), X-ray diffraction (XRD), and Fourier-transform infrared (FTIR) spectroscopy. Ten specimens were tested per formulation in each mechanical assay (five initial specimens and five confirmatory specimens), and the mechanical data were consolidated across all ten specimens and are reported as an arithmetic mean ± standard deviation (SD). The recorded response was loading-mode-dependent: PLA-5Mg-5nHA combined a tensile stress of 52.0 ± 1.56 MPa with the largest tensile peak displacement ratio of 23.42 ± 0.70%; PLA-7.5Mg-2.5nHA showed the largest flexural peak load of 490.4 ± 14.71 N; and PLA-2.5Mg-7.5nHA combined 52.8 ± 1.58 MPa tensile stress, 93.7 ± 2.81 MPa compressive stress, and 431.5 ± 12.95 N flexural peak load. DSC showed a high-temperature heat-flow event at 365.6-372.6 °C under the stated mixed-purge conditions; this is treated as an operational thermal marker and not a melting or decomposition temperature. XRD remained matrix-dominated with reinforcement-sensitive features, while FTIR showed composition-dependent shifts in the C-O/C-O-C region. The results indicate that Mg:nHA partitioning alters the recorded loading-mode response within the tested 10 wt.% reinforcement window, while particle-scale mechanisms and biological performance require further validation.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Polylactic acid/hydroxyapatite composite filaments: Balancing printability, mechanical integrity, and osteogenic performance for bone tissue engineering.International journal of biological macromolecules · 2026
- Development and Characterization of PLA/PEG/Flax Bio Composites: Influence of Fiber Treatment and Plasticizer Content for Bone-Related Bioengineering ApplicationsApplied Sciences · 2026
- Beyond Reinforcement: A Critical Review of Process–Structure–Property Relationships in Additively Manufactured PLA CompositesJournal of Composites Science · 2026
- 3D Printing and Characterization of HA/Mg-Reinforced PLA–PHA–PHB Composite Scaffolds for Biomedical ApplicationsApplied Sciences · 2026
- Polylactic Acid Hybrid Composites Reinforced with Thermally Modified Wood Flour and Cellulose NanofibrilsApplied Sciences · 2026
- Fabrication and evaluation of PLA/PA-HA filament for 3D printing: towards trabecular bone-compatible biomedical applicationsThe International Journal of Advanced Manufacturing Technology · 2025