Effect of Acid-Labile Protecting-Group Structure on the Micrometer-Scale Patterning Performance of Core-First RAFT-Synthesized Three-Arm Photoresists.
Jinyoung Kim, Yura Choi, Eunsu Park, Kyeongjin Jang, Hyungjun Noh, Namchul Cho
Department of Energy Engineering, Soonchunhyang University, 22 Soonchunhyang-ro, Asan 31538, Republic of Korea.
Key points
From the paper's conclusion- These results indicate that an acid-labile protecting-group structure can influence thermal behavior and micrometer-scale pattern fidelity within the investigated three-arm RAFT polymer platform.
Abstract
Controlling dimensional fidelity and line-edge roughness is important in chemically amplified negative-tone imaging. In this study, two three-arm random terpolymers containing different acid-labile protecting groups were synthesized via core-first reversible addition-fragmentation chain-transfer (RAFT) polymerization to examine the influence of protecting-group structure within a common star-polymer framework. HTT 334 contained tert-butyl methacrylate (t-BMA), whereas HTM 334 contained 2-methyl-2-adamantyl methacrylate (MAMA). The two polymers exhibited comparable molecular weights and compositions, with narrow dispersities of 1.14 and 1.16. Thermal analysis showed that HTM 334 had a slightly higher glass-transition temperature than HTT 334 (77 and 73 °C, respectively). Fourier transform infrared (FT-IR) spectroscopy revealed spectral changes after exposure and post-exposure baking (PEB) that were consistent with acid-catalyzed deprotection and possible intermolecular reactions involving the hydroxyethyl methacrylate units. Negative-tone patterns were formed using an n-butyl acetate developer under the selected PEB conditions of 70 °C for HTT 334 and 90 °C for HTM 334. Across nominal mask dimensions of 10-80 μm, HTM 334 exhibited printed-to-mask critical-dimension ratios of 0.990-1.039, compared with 0.915-1.003 for HTT 334. HTM 334 also showed lower measured line-edge roughness values of 0.22-0.39 μm than HTT 334, which showed values of 0.52-1.27 μm. At the nominal 10 μm dimension, HTM 334 exhibited a line-edge roughness of 0.27 μm and an LER/CD ratio of 2.60%. These results indicate that an acid-labile protecting-group structure can influence thermal behavior and micrometer-scale pattern fidelity within the investigated three-arm RAFT polymer platform.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Composition-Dependent Lithographic Performance of 3-Arm Star Photoresists.Polymers · 2026
- Influence of Trifunctional RAFT Chain-Transfer-Agent-Mediated Polymerization Conditions on the Negative-Tone Patterning Behavior of Methacrylate-Based PhotoresistsJournal of Manufacturing and Materials Processing · 2026
- Rational Design of Degradable Multiarm Polymers Applicable for Photoimaging MaterialsChemistry of Materials · 2026
- Synthesis of Poly(4-hydroxystyrene) for Photoresist: Nitroxide-Mediated Polymerization and Homogeneous Acidic Hydrolysis.ACS omega · 2026
- Exposure dose-dependent multi-tone photolithography via photoacid-induced crosslinking and degradation of poly(2,3-dihydrofuran).Nature communications · 2026
- RAFT-Mediated 3D Printing of Polylactones/Itaconate Elastomers with Polypeptide Surface FunctionalizationACS Polymers Au · 2025