Effect of Different PTFE Coatings Applied to 18CrNiMo7-6 Steel on the Coefficient of Friction and Wear Under Dry Sliding Contact Using the Ball-on-Disk Method at Different Loads.
Michal Krbata, Marcel Kohutiar, Mariana Janeková, Branislav Hoferica, Daniel Krizan, Jana Escherova, Andrej Dubec, Bohdan Trembach,
Faculty of Special Technology, Alexander Dubcek University of Trenčín, 911 06 Trenčín, Slovakia. · Faculty of Industrial Technologies in Púchov, Alexander Dubček University of Trenčín, Ivana Krasku 491/30, 020 01 Púchov, Slovakia.
Key points
From the paper's conclusion- Overall, Xylan® 1425 provided the best balance of low friction, mechanical stability, coating continuity, and wear resistance.
Abstract
This study investigates the tribological performance of three commercial PTFE-based Xylan® coatings-Xylan® 1425, Xylan® 1052, and Xylan® 1010-applied to 18CrNiMo7-6 steel under dry sliding conditions. Ball-on-Disk tests were conducted at normal loads of 5, 7.5, and 10 N, wear-track radii of 12, 16, and 20 mm, and corresponding sliding velocities of 0.31-0.52 m·s-1. The tribological evaluation was complemented by measurements of coating thickness, surface roughness, nanoindentation, wear-track profilometry, scanning electron microscopy, EDS mapping, and post-test cross-sectional microscopy. All coatings reduced the coefficient of friction from approximately 0.49-0.64 for the uncoated steel to 0.09-0.13, corresponding to an average reduction of 78-80%. Xylan® 1425 exhibited the highest nanohardness of 57.02 MPa, the highest reduced elastic modulus of 3.33 GPa, and the most favorable elastoplastic indices. It also achieved the lowest wear, with a volumetric loss of approximately 0.03 mm3 under the most severe conditions, representing a reduction of more than 99% compared with the substrate. Xylan® 1010 provided the lowest friction but showed pronounced plastic deformation, whereas Xylan® 1052 exhibited fragmentation and increased wear. Post-test cross-sectional microscopy confirmed local exposure of the steel substrate in both coatings. Overall, Xylan® 1425 provided the best balance of low friction, mechanical stability, coating continuity, and wear resistance.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Metric‐Dependent Friction and Wear Rankings of Polyalkylene Glycol LubricantsJournal of Tribology · 2026
- Preparation and tribological properties of filler-reinforced PTFE/PPS coatings deposited on textured surfacesSurface Topography Metrology and Properties · 2026
- Tribological Properties and Mechanisms of PTFE Matrix Composites Under Wide‐Temperature‐Range and Long‐Term Friction ConditionsPolymer Composites · 2026
- Effect of Counter-Surface Texturing on the Tribological Behavior of Virgin and Glass-Filled Polytetrafluoroethylene During Sliding Against Grey Cast Iron.Polymers · 2026
- Study on the Optimization of Tribological Properties of Ductile Iron by Micro‐Texture and Solid Lubrication CoatingsLubrication Science · 2026
- Improving Self‐Lubricating Performance of AISI 4140 Steel Composites Reinforced With Nickel‐Coated Multi‐Walled Carbon Nanotubes Under Dry Sliding ConditionsJournal of Tribology · 2026