Upcycling Waste Expanded Polystyrene into Fe@Graphitic-Carbon Catalysts for Glycolytic Recycling of PET to BHET.
Jong In Choi, Chitra Sarkar, Yujin Kang, Saira Kanwal, Youn-Sang Bae, Do-Young Hong
Research Center for Nanocatalysts, Korea Research Institute of Chemical Technology (KRICT), 141 Gajeong-ro, Yuseong, Daejeon 34114, Republic of Korea. · Department of Chemical and Biomolecular Engineering, Yonsei University, 50 Yonsei-ro, Seodaemun-gu, Seoul 03722, Republic of Korea.
Key points
From the paper's conclusion- The data support a two-stage pathway in which external graphitic carbon/CNT domains promote primary PET chain scission to soluble oligomers, followed by Fe@C interfacial secondary glycolysis to BHET.
Abstract
Chemical glycolysis can convert waste poly(ethylene terephthalate) (PET) into bis(2-hydroxyethyl) terephthalate (BHET), but recyclable heterogeneous catalysts derived from circular carbon sources and showing low metal release remain limited. Here, post-consumer expanded polystyrene (EPS) was transformed into a hypercrosslinked polymer (HCP) and carbonized with Fe to produce Fe@graphitic-carbon (Fe@C) catalysts for PET glycolysis. The catalysts are denoted mFe@EPS-HCP800, where m represents the nominal Fe loading (wt.%), and 800 is the carbonization temperature (°C). The optimized 5Fe@EPS-HCP800 contained graphitic carbon layers, bamboo-like carbon nanotube (CNT) domains, hierarchical porosity, and Fe-rich domains associated with graphitic carbon coverage. Under atmospheric-pressure conditions (PET, 2.00 g; ethylene glycol, 20.00 g; catalyst, 0.20 g; 200 °C; 2 h), it achieved complete PET conversion and 94.6% BHET yield. The catalyst also maintained BHET yields of ca. 90-94% over ten reuse runs, and post-reaction microscopy confirmed the retention of graphitic carbon layers and Fe-containing domains. Fe was below the detection limit in the product solutions for the 1, 3, and 5 wt.% Fe catalysts, whereas 7Fe@EPS-HCP800 released 9.1 mg kg-1 Fe, consistent with incomplete carbon coverage at excessive Fe loading. Conversion profiles followed an Avrami-Erofeev/Weibull model, giving an apparent activation energy of 205.6 kJ mol-1. The data support a two-stage pathway in which external graphitic carbon/CNT domains promote primary PET chain scission to soluble oligomers, followed by Fe@C interfacial secondary glycolysis to BHET. This work demonstrates dual waste-polymer valorization by using EPS waste as catalytic infrastructure for PET chemical recycling.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Efficient Glycolysis of Polyethylene Terephthalate (PET) Catalyzed by Cyclic(alkyl)(amino)carbene Copper ComplexesMolecules · 2025
- Glycolysis of Waste Poly(ethylene Terephthalate) Through Acid–Base Cooperative CatalysisChemSusChem · 2026
- Efficient Glycolysis of Waste PET at Room Temperature Enabled by a Bifunctional Catalyst System and Co-solventACS Sustainable Resource Management · 2026
- Bioconversion of ethylene glycol to glycolic acid for waste polyethylene terephthalate upcyclingGreen Chemistry · 2026
- Selective Upcycling of Waste PET into Di(2-ethylhexyl) Terephthalate via a Hybrid Organometallic Catalytic Strategy for PVC Plasticizer Applications.Polymers · 2026
- Inorganic/Organic Hybrid Magnetic Nanocatalysts for Effective PET GlycolysisACS Sustainable Chemistry & Engineering · 2026