In Situ Synthesis, Crystallization Behavior and Mechanical Properties of Biodegradable Poly(Ethylene Succinate)/Talc Composites.
He Yang, Siyu Pan, Zhaobin Qiu
State Key Laboratory of Chemical Resource Engineering, Beijing University of Chemical Technology, Beijing 100029, China.
Key points
From the paper's conclusion- Although the mechanical properties of PES/talc2.0 (2 wt% talc) were inferior to those of neat PES and the other two composites, it still displayed relatively good mechanical properties.
Abstract
Poly(ethylene succinate) (PES) is a promising biodegradable polyester with excellent thermal and mechanical properties; however, slow crystallization rate has seriously restricted its widespread application. PES/talc composites at low talc contents of 0.5 to 2.0 wt% were synthesized via an in situ polymerization method in this research. The chemical structure, thermal stability, crystallization behavior, crystalline morphology, crystal structure, and tensile mechanical properties of PES/talc composites were extensively investigated with various techniques and compared with those of neat PES. Talc remarkably enhanced the crystallization behavior of PES under different crystallization conditions as an effective nucleating agent. For instance, 2 wt% talc increased the melt crystallization temperature of PES from 46.1 to 58.9 °C at a cooling rate of 5 °C/min and shortened the crystallization half time to 1.95 min from 7.69 min at 66 °C. However, talc remained the crystallization mechanism and crystal structure of PES. The nucleation mechanism of talc on the crystallization of PES was further discussed. The exact nucleation mechanism was still uncertain, which needs further investigation. The mechanical properties of PES/talc composites were dependent on the talc content. For instance, 0.5 and 1 wt% talc decreased the tensile strength values to 34.1 ± 1.9 and 33.7 ± 2.1 MPa from 44.9 ± 1.3 MPa, while the elongation at break values increased to 675.3 ± 24.8% and 560.4 ± 11.9% from 508.0 ± 13.4%, respectively, indicating an increase in toughness. Although the mechanical properties of PES/talc2.0 (2 wt% talc) were inferior to those of neat PES and the other two composites, it still displayed relatively good mechanical properties.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Homogeneously Blending PBAT with Silanized Cellulose for Composite Film: Characterization and Physicochemical PropertyPolymers · 2026
- Investigating the Crystallization Kinetics and Mechanical Properties of Poly(Butylene Succinate): The Dual Role of Polyoxymethylene Blending and MWCNT Heterogeneous Nucleation.Polymers · 2026
- Stereocomplex crystallite-mediated modification of poly(lactic acid)-based composites.International journal of biological macromolecules · 2026
- Influence of PDMS Molecular Weight on Isothermal Crystallization in PDMS and PDMS-Zeolite Composites: A DSC and ESR Spin Probe Study.Polymers · 2026
- A Recyclable Polythioester With α ‐Gem‐Dimethyl Substitution: Instantaneous Crystallization Triggered by Large and Rapid StretchingAdvanced Materials · 2026
- Direct Pellet Extrusion of Calcined Seashell Particle Reinforced Polylactic Acid CompositePolymer Composites · 2026