Dual Effects of Thermal Annealing on Rotomolded PLA Biocomposites: A Fiber-Content Study.
Erick Omar Cisneros-López, Josué Rivera-Aguilera, Rosa Gabriela López-Gonzaleznúñez, Pedro Ortega-Gudiño, Rubén González-Núñez, Esperanza González-Quezada, Roberto Carlos Vázquez-Fletes
Centro Universitario de Ciencias Exactas e Ingenierías (CUCEI), Universidad de Guadalajara, Blvd. Gral. Marcelino García Barragán #1421, Guadalajara C.P. 44430, Mexico. · Departamento de Estado Sólido, Instituto de Física, Universidad Nacional Autónoma de México (UNAM), Ciudad de México C.P. 01000, Mexico.
Key points
From the paper's conclusion- This work evaluates annealing at 100 °C for 1 h on rotomolded PLA biocomposites reinforced with 10, 20, and 30 wt.% of agave, coir, or pine fibers.
Abstract
Rotational molding is a shear-free technology to produce hollow plastic parts. Rotomolded poly(lactic acid) (PLA) and its biocomposites remain in a largely amorphous state, which limits their stiffness, toughness, and thermal resistance. Post-processing thermal annealing develops crystallinity without additives, but its combined effect with natural fibers has rarely been quantified. This work evaluates annealing at 100 °C for 1 h on rotomolded PLA biocomposites reinforced with 10, 20, and 30 wt.% of agave, coir, or pine fibers. Crystallinity (DSC, XRD), density and porosity, morphology (SEM), water absorption, mechanical properties (tensile, flexural, Charpy impact, Shore D hardness), and 28-day disintegration under lab-scale composting conditions were measured for treated and untreated samples. Annealing raised the matrix crystallinity from below 21% to 41-56% and produced predominantly α crystals with a nearly constant average size of about 20 nm. The treatment improved the matrix-dominated properties for every formulation: for neat PLA, Charpy impact strength increased by 120% (28.1 to 61.7 J/m), flexural strength by 53% (61.1 to 93.4 MPa), and flexural modulus from 3264 to 4511 MPa. Tensile strength and modulus, in contrast, remained unchanged or decreased. Porosity, set by fiber content, was unaffected by annealing; at 30 wt.%, the matrix barrier nonetheless reversed, and annealed samples absorbed more water and disintegrated faster than untreated ones. Fiber content sets the balance between matrix crystallinity and the interfacial damage caused by crystallization-induced contraction.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Post-Print Annealing of FDM-Printed Polylactic Acid: Mapping Strength, Crystallinity, and α′/α Polymorph Composition via a Replicated Taguchi L9 DesignPolymers · 2026
- Effect of Annealing on the Mechanical Properties of Carbon Fiber-Reinforced PLA.Polymers · 2026
- Effect of post-printing annealing on the tensile behavior of stainless-steel wire mesh–reinforced PLA composites fabricated using material extrusionAdvances in Mechanical Engineering · 2026
- Vacuum and Non-Vacuum Hydrothermal Annealing as a Post-Processing of MEX PLA on Tensile Response and Fracture Characteristics.Polymers · 2026
- Thermal, Mechanical, and Rheological Properties of PLA/PHB Biocomposites Reinforced with Alkaline-Treated Hemp Fibers and GranulesChemEngineering · 2025
- Development and Characterization of PLA/PEG/Flax Bio Composites: Influence of Fiber Treatment and Plasticizer Content for Bone-Related Bioengineering ApplicationsApplied Sciences · 2026