Mechanical and Microstructural Response of FDM-Printed PETG and PETG+CF to Variable Infill Architecture and Lubricant Exposure
Lidija Rihar, Elvis Hozdić
Higher Education Centre Novo Mesto
Key points
From the paper's conclusion- This study quantifies the combined influence of (i) infill pattern (linear, triangular, hexagonal) at 30% density, (ii) infill density (30%, 60%, 100%) for linear infill, and (iii) short-term lubricant exposure on the tensile and microstructural response of FDM-printed polyethylene terephthalate glycol-modified (PETG) and short-carbon-fibre-reinforced PETG (PETG+CF).
Abstract
Fused deposition modelling/fused filament fabrication (FDM/FFF) enables rapid manufacturing of functional polymer components; however, the reliability of printed parts remains strongly governed by internal architecture, process-induced porosity, and exposure to service fluids. This study quantifies the combined influence of (i) infill pattern (linear, triangular, hexagonal) at 30% density, (ii) infill density (30%, 60%, 100%) for linear infill, and (iii) short-term lubricant exposure on the tensile and microstructural response of FDM-printed polyethylene terephthalate glycol-modified (PETG) and short-carbon-fibre-reinforced PETG (PETG+CF). Specimens were printed following ISO 527-2 and tensile-tested at 5 mm/min. Microstructural analysis coupled quantitative porosity with mechanical response, Young's Modulus, and strain-to-break. At 30% density, PETG with hexagonal infill achieved the highest tensile strength (18.54 ± 0.67 MPa), exceeding linear (16.99 ± 0.52 MPa) and triangular (14.15 ± 0.70 MPa) patterns, while triangular and linear patterns exhibited higher Young's Modulus, indicating topology-driven decoupling of stiffness and strength. Increasing linear infill density raised strength to 31.35 ± 0.33 MPa (PETG) and 38.90 ± 0.28 MPa (PETG+CF) at 100%, consistent with reduced porosity. Seven-day immersion in SAE 15W-40 mineral engine oil reduced PETG strength by ~17% while increasing deformation to failure, whereas PETG+CF showed only minor changes. Overall, the results demonstrate that architecture-aware design, supported by quantitative porosity descriptors, is essential for ensuring the reliable mechanical performance of FDM/FFF-printed PETG-based components exposed to service fluids.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Mechanical Parameters and Microstructural Evolution of FDM-Printed PLA and PLA+CF Under Variable Infill Architecture and Lubricant ExposurePolymers · 2025
- Optimizing the Mechanical Performance of 3D-Printed PLA, ABS, and PETG Through Infill Density and PatternJournal of Manufacturing and Materials Processing · 2026
- Optimization of 3D Printing Parameter Effects on Mechanical Properties in Polyethylene Terephthalate Glycol (PETG) Filament Production Using FDM and Response Surface MethodologyPolymers · 2026
- Influence of Infill Density on Bacterial Colonization and Mechanical Performance of 3D-Printed PETG Scaffolds.Polymers · 2026
- Reinforcement of Novel PLA/17-4 PH Stainless Steel Hybrid Structures Fabricated by FDM: The Effects of Layer Configuration, Infill Density and PatternPolymers · 2026
- Tribo-mechanical performance and microstructural characterization of FDM printed PLA and ABS componentsJournal of Materials Research and Technology · 2026