Increasing the Service Life of Solid Ceramic End Mills by Treating Their Surfaces with Fast Argon Atoms
Alexander S. Metel, Marina A. Volosova, Anna A. Okunkova, Enver S. Mustafaev, Yury A. Melnik, Sergey N. Grigoriev
Key points
From the paper's conclusion- The combined treatment of SiAlON ceramic end mills comprising the removal of a 5 µm thick surface layer and subsequent deposition of a 3 µm thick wear-resistant coating significantly reduces tool wear and increases the average tool life by 1.7 times compared to untreated mills.
Abstract
Commercially available solid ceramic end mills, which are remarkable for producing high-quality machined surfaces and achieving cutting speeds unattainable with tungsten carbide tools, are characterized by a wide range of mean times between failures, indicating their low reliability. The primary cause is surface defects generated by diamond grinding during the manufacturing of the mills. In the present study, it is proposed to remove the defective layer by sputtering it with a beam of fast argon atoms, which at the same time appreciably sharpens the cutting edges of the mill. The combined treatment of SiAlON ceramic end mills comprising the removal of a 5 µm thick surface layer and subsequent deposition of a 3 µm thick wear-resistant coating significantly reduces tool wear and increases the average tool life by 1.7 times compared to untreated mills.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Optimized surface morphological characterization employing LASER-drilled hole to enhance the EDM efficiency of MoSi₂ -SiC intermetallic compositesMaterials Science and Technology · 2026
- Cutting Performance of SiAlON Ceramic End Mills in the High-Speed Milling of Inconel 718Coatings · 2026
- Ultrasonic Vibration-Assisted Micro-Electrical Discharge Machining Characteristics and Parameter Optimization of C/SiC CompositesMicromachines · 2025
- Reducing tool wear in high-speed milling of Inconel 718 by optimizing flank-face coolant direction: A CFD-supported approach toward sustainable machiningJournal of Manufacturing Processes · 2026
- Atomic-scale removal mechanism of chemically enhanced diamond turning of single crystal silicon carbidenpj Advanced Manufacturing · 2026
- Formation mechanism of grinding wheel oxide layer in the ultrasonic-assisted ELID grinding of silicon carbide ceramicsUltrasonics Sonochemistry · 2026