Annealing-Induced Structural, Optical, and Electrical Tuning of Sputtered Ge-Doped ZnO Thin Films for Transparent Conducting Applications
Dur-e-Shehwar Kiyani, Shaista Shahzada
Key points
From the paper's conclusion- Ge-doped ZnO thin films were fabricated using the RF magnetron sputtering system on Si and glass substrates at room temperature, followed by post-deposition annealing at various temperatures to investigate the effects of annealing on the structural, optical, and electrical properties of the films.
Abstract
Ge-doped ZnO thin films were fabricated using the RF magnetron sputtering system on Si and glass substrates at room temperature, followed by post-deposition annealing at various temperatures to investigate the effects of annealing on the structural, optical, and electrical properties of the films. The X-ray diffraction results show that all the films are polycrystalline and have a hexagonal wurtzite structure. The crystallite size of the film was found to increase after annealing at 650 °C. The wurtzite structure of ZnO was further confirmed by Raman scattering with a dominant band at 435–438 cm−1 corresponding to the E2 (high) phonon mode. The presence of the Zn–O framework and a Ge-related vibrational band at 565 cm−1 was confirmed by FTIR, which is in line with Ge–O bonding and Ge incorporation; no crystalline impurity phase could be found in the range of XRD and Raman sensitivity. The film was annealed at 650 °C and then analyzed by XPS, which revealed chemical states of Zn2+ and Ge4+ with no evidence of the presence of metallic Ge. The optical transmittance was at its maximum at the best-performing temperature, 650 °C, at which the optical band gap (Eg) of the film increased from 3.45 eV to 3.57 eV. Spectroscopic ellipsometry showed that both the refractive index and extinction coefficient changed smoothly with the annealing temperature. The carrier concentration of the film annealed at 650 °C was measured to be 4.71 × 1020 cm−3, with a mobility of 39 cm2/V.s, and resistivity of 3.40 × 10−4 (Ω·cm), corresponding to a Haacke figure of merit of 5.1 × 10−2 Ω−1. Some modest visible light photo-switching was observed in a photoresponse measurement under 555 nm illumination (preliminary data).
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Annealing induced bandgap engineering and interfacial oxide formation in nanostructured TiO 2 -Ge thin film heterojunctions for photovoltaic applicationsPhysica Scripta · 2026
- Sol–gel derived ITO thin films with (400) preferred orientationDiscover Materials · 2026
- Nonequilibrium Dopant Activation and Emission Wavelength Modulation in Heavily Sb-Doped Ge(Si) Thin Films by High-Speed Continuous-Wave Laser AnnealingACS Applied Electronic Materials · 2026
- Annealing-Temperature-Dependent Electrical and Optical Performance of Solution-Processed Amorphous IGZO TFTsTechnologies · 2026
- Air-annealing-induced vertical elemental gradients regulate defect chemistry and optoelectronic properties of cylindrical-target-sputtered ITO thin films.RSC advances · 2026
- Engineering CZTS thin film properties via Ag and Ge co-dopingJournal of Materials Science Materials in Electronics · 2026