Electrical Resistance Behavior of Printed Ag Nanowire Electrode Lines Under Transverse Tensile Strain.
Yoon Jae Moon, Jiyeong Kong, Sukkee Um, Kyung-Tae Kang
Autonomous Manufacturing & Process R&D Department, Korea Institute of Industrial Technology, 143 Hanggaul-ro, Sangnok-gu, Ansan-si 15588, Republic of Korea. · School of Mechanical Engineering, Hanyang University, 222 Wangsimni-ro, Seongdong-gu, Seoul 04763, Republic of Korea.
Key points
From the paper's conclusion- These results indicate an intermediate response at 20% strain and a clear transition to a network-damage-dominated response at 30% strain.
Abstract
Printed stretchable interconnects may experience tensile deformation perpendicular to the direction of current flow, but their electrical response under transverse loading remains insufficiently understood. In this study, dispenser-printed silver nanowire (Ag NW) line electrodes on polydimethylsiloxane were subjected to transverse tensile strains of 10-40% for 10 stretching-release cycles. Ten specimens were tested at each strain level. Resistance was measured in situ, and deformation-induced changes in the Ag NW network were examined using optical microscopy and field-emission scanning electron microscopy (FESEM). To distinguish the effects of macroscopic deformation from changes in network connectivity, the measured resistance was compared with geometric predictions based on Poisson-induced shortening of the printed line. At 10% strain, the stretched-state resistance closely followed the geometric prediction and remained nearly unchanged during cycling. At 20% strain, the resistance increased progressively with repeated cycling and local cracks were observed, whereas the first-cycle deviation from the geometric reference remained small relative to the specimen-to-specimen variation. At 30% and 40% strain, the measured resistance clearly exceeded the geometric reference in both the stretched and released states. After 10 cycles at 40% strain, the corresponding relative resistances reached 1.369 and 1.736, respectively. FESEM observations showed that conductive nanowire bridges remained across locally cracked regions at 20% strain, whereas crack penetration into the line interior and local pathway loss were observed at 30% strain. These results indicate an intermediate response at 20% strain and a clear transition to a network-damage-dominated response at 30% strain.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Predictive modeling of optical and electrical coupling in silver nanowire networks for stretchable transparent electrodesNanoscale · 2026
- Silver Nanowire for Mechanically Durable Electroluminescent Devices and Stretchable Printed CircuitsChemNanoMat · 2026
- Supramolecular Pulley Effect Enabling Highly Stretchable Transparent Electrodes.ACS applied materials & interfaces · 2026
- Silver Nanowire-Based Flexible Transparent Electrodes: Fabrication and ApplicationsCoatings · 2026
- Liquid Metal and Silver Nanowires Synergic Network-Enabled Triboelectric Fiber for Strain-Insensitive Multifunctional ApplicationsAdvanced Fiber Materials · 2025
- 2D Silver Nanosheet Assembly for an Isotropic, Stretchable, and Highly Conductive NanomembraneAdvanced Materials · 2025