Key points
From the paper's conclusion- Together, these results identify chain termination and segment orientation as candidate design variables and provide quantitative descriptors for morphology-matched thermal comparisons and orientation-resolved electronic screening.
Abstract
Identifying the molecular origins of thermal and electric-field response can guide polyimide insulation design. We combined an 18-film aromatic imide oligomer ensemble, reactive molecular dynamics, and signed finite-field r2SCAN-3c calculations to separate packing, chain-end chemistry, and directional electronic response. Independently initialized films exhibited a fivefold variation in probe-accessible volume, with distinct connected void geometries at similar accessible fractions. Across sixteen 5 ps thermal trajectories, terminal imide N-H sites accounted for 20 of 21 persistent reference-bond losses; the nonterminal inventory contained 14 new C-O connectivities and one C-N loss. In six matched film pairs, nonterminal records increased from 2 to 5 at 1600 K and from 12 to 19 at 1800 K between 5 and 10 ps, revealing the growing contribution of nonterminal rearrangement. Trajectories extending to 20 ps also resolved the onset of increased mass escape. At ±2 V nm-1, the isolated ether-linked bis-imide fragment showed 0.342-0.841 eV frontier-gap narrowing across six directions, compared with at most 0.049 eV for the imide fragment, despite overlapping size-normalized induced responses. Together, these results identify chain termination and segment orientation as candidate design variables and provide quantitative descriptors for morphology-matched thermal comparisons and orientation-resolved electronic screening.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Fatigue‐Resistant Mechanically Interlocked Co‐Crosslinked Polyimide Films for Reliable High‐Temperature Capacitive Energy StorageAdvanced Functional Materials · 2026
- Optimizing High-Temperature Energy Storage Performance of Polyetherimide by Biaxial Orientation Stretching.Small (Weinheim an der Bergstrasse, Germany) · 2026
- High-Temperature Energy Storage in Semi-Aromatic Polyimide with Dual Crosslinking NetworksMaterials Futures · 2026
- Main-Chain Linkage Effects on Field-Induced Conformation and High-Frequency Dielectric Dissipation in PolyimidesACS Applied Polymer Materials · 2026
- Tuning Diamine Architecture in 6FDA-Based Polyimides for Enhanced High-Temperature Capacitive Energy StorageACS Applied Energy Materials · 2026
- Thermally self-crosslinkable polyetherimide dielectrics with superior high-temperature energy storage efficiencyJournal of Materials Chemistry A · 2026