Tuning Molecular Weight for Transparent Negative-Tone Photosensitive Polyimide
Lili Yuan, Jiaxin Ma, Wei Chen, Lizhe Wang, Shiyong Yang, Haixia Yang
Key points
From the paper's conclusion- To investigate the effect of poly(amic ester) (PAE) molecular weight on the photolithographic performance of negative-tone photosensitive poly(amic ester)s (n-PSPAE) and the comprehensive properties of cured negative-tone photosensitive polyimide films (n-PSPI), a series of molecular-weight-controlled PAE resins functionalized with photoreactive hydroxyethyl methacrylate (HEMA) moieties were prepa
Abstract
To investigate the effect of poly(amic ester) (PAE) molecular weight on the photolithographic performance of negative-tone photosensitive poly(amic ester)s (n-PSPAE) and the comprehensive properties of cured negative-tone photosensitive polyimide films (n-PSPI), a series of molecular-weight-controlled PAE resins functionalized with photoreactive hydroxyethyl methacrylate (HEMA) moieties were prepared via a three-step esterification–acyl chlorination–polycondensation route. This route used 4,4′-(hexafluoroisopropylidene)diphthalic anhydride (6FDA) and 3,3′,4,4′-biphenyltetracarboxylic dianhydride (BPDA) as the mixed dianhydrides and 2,2′-bis(trifluoromethyl)benzidine (TFDB) as the diamine. Viscous n-PSPAE solutions were then formulated by dissolving PAEs along with photoinitiators, photocrosslinkers, polymerization inhibitors, and adhesion promoters in N-methyl-2-pyrrolidone (NMP). As PAE theoretical molecular weights (Mwcalc) increase, the gelation threshold energy density (D0.5) decreases from 118 to 44 mJ·cm−2 due to reduced dissolution kinetics in the developer. Optimized spatial resolutions of 6–8 μm for vias and lines are retained at Mwcalc ≤ 30 × 103 g·mol−1 (with n-PSPAE-2–20 reaching 6 μm for both geometries), beyond which developer-induced swelling severely degrades the pattern definition. The thermal, mechanical, dielectric, and optical properties of n-PSPI films cured at 350 °C were systematically investigated as a function of PAE Mwcalc. The fully cured n-PSPI films demonstrate exceptional thermal and thermomechanical endurance, where PAE Mwcalc plays a negligible role in altering primary pyrolytic degradation stability and thermal expansion, owing to the intrinsically rigid aromatic backbone. Correspondingly, a minimum precursor Mwcalc of approximately 25 × 103 g∙mol−1 is required to enter the chain entanglement transition region, ensuring high tensile strength and elongation at break. And an optimum practical window of 25 × 103–30 × 103 g∙mol−1 balances fine micro-patterning with mechanical reliability. Furthermore, the n-PSPI films combine exceptionally stable low dielectric constants, minimal loss, and outstanding optical clarity, with T550 values of 93.6–95.4%, a haze of ≤0.97%, and a yellowness index of 5.79–11.88. These excellent properties originate from the suppression of intermolecular charge transfer complexes and increased fractional free volume induced by bulky fluorinated groups.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Synthesis and Properties of a Biophenolic End-Capped Polyimide Photoresist with High Film Retention and SensitivityACS Applied Polymer Materials · 2026
- Fluorine-Free, Low-Dielectric Photosensitive Polyimides Based on Methyl Methacrylate-Functionalized Bulky Diamines for High-Fidelity UV PatterningACS Applied Polymer Materials · 2026
- A Molecular Design Strategy for Biobased, Fluorine-Free, Aqueous-Developable, and Positive-Type Photosensitive Polyimides with Low Dielectric Loss at High Frequencies of 10–40 GHzACS Applied Polymer Materials · 2026
- Synthesis and Properties of Semi-Alicyclic Polyimides Based on an Asymmetric Diamine from Renewable Menthofuran.Polymers · 2026
- Facile Strategy Enabling Fluorine-Free Polyimides with Ultralow Dielectric Loss and Thermal Expansion Close to CopperACS Applied Materials & Interfaces · 2026
- Research on the Synthesis and Characterization of Colorless Polyimide Based on a Novel Asymmetric Dianhydride MonomerACS Omega · 2026