Department of Glass Technology and Amorphous Coatings, Faculty of Materials Science and Ceramics, AGH University of Krakow, Al. Mickiewicza 30, 30-059 Krakow, Poland. · Department of Animal Biotechnology, Faculty of Animal Sciences, University of Agriculture in Krakow, A. Mickiewicz 24/28 Av., 30-059 Krakow, Poland.
Key points
From the paper's conclusion- The results support wool–PLA mats as temporary, degradable carriers of keratin-bound sulphur; replicated field trials with yield, nutrient uptake and soil measurements, together with direct degradation markers, are required before any fertilising or soil-improving effect can be claimed.
Abstract
Low-grade sheep wool is an underused, keratin-rich by-product whose cystine-derived sulphur could be returned to agricultural soils. Carded wool was bonded with sprayed poly(lactic acid) (PLA) hot-melt to obtain porous wool-PLA biocomposite mats, which were exposed in field soil, in a pasture-grass composter and under soil-free outdoor conditions. The elemental composition of the wool, soil, forage, composting material and exposed mats was determined by ICP-OES after 60 days of exposure; each reported value is the mean of at least three analytical determinations, whereas the field layout comprised one plot per treatment. Forage from the plot with buried mats contained 47.8% more S and 21.9% more K than forage from the untreated plot, whereas Ca, Mg, B and Mo concentrations were lower; because the plots were not replicated, these differences are reported as preliminary observations rather than as demonstrated treatment effects. After composting, the mats retained only 17-23% of their initial storage modulus between -30 and 50 °C, while the relaxation of the PLA phase shifted by 7-10 °C towards higher temperatures. The water contact angle decreased from 72.3 ± 10.0° to 55.7 ± 12.1° (six droplets on one mat per condition), while the stylus roughness did not change appreciably. Digital microscopy revealed swelling, fissuring, cavities and fibre exposure along wool-PLA interfaces. A coupled mechanism of PLA ester hydrolysis and keratinolytic release of sulphur is proposed as a working hypothesis that is consistent with, but not yet proven by, the present data. The results support wool-PLA mats as temporary, degradable carriers of keratin-bound sulphur; replicated field trials with yield, nutrient uptake and soil measurements, together with direct degradation markers, are required before any fertilising or soil-improving effect can be claimed.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Long-Term Environmental Durability of Recycled Textile-Low-Density Polyethylene Composites Reinforced with Plant Fibers: Mass Uptake, Flexural Stability, and Microbial Colonization.Materials (Basel, Switzerland) · 2026
- Biodegradation behavior of waste cotton fiber-reinforced polylactic acid composites under soil-burial conditionsProceedings of the Institution of Mechanical Engineers Part L Journal of Materials Design and Applications · 2026
- Tensile characterization and life cycle assessment of fungal-colonized 3D-printed PLA/wood biocomposites.Scientific reports · 2026
- Developing High‐Performance Biodegradable Poly(Butylene Succinate) Composites Through Synergistic Effects of Fiber Surface Mineralization and Soybean Protein Bonding Onto Sisal Woven FabricsPolymer Composites · 2026
- Investigation of Porosity and Cell Wall Swelling in Sisal Yarn Reinforced Polylactic Acid CompositesPolymer Composites · 2026
- Posidonia oceanica Leaves as a Natural Filler for Poly(Butylene Succinate‐Co‐Adipate) Composites: Characterization and Biodegradation Assessment in SeawaterJournal of Vinyl and Additive Technology · 2026