Gd3+-Driven Microstructure Regulation of Tm3+, Yb3+: GdxBi2-xWO6 for High-Sensitivity Temperature Sensing and Magnetism.
Xin Feng, Linxiang Wang, Jiachen Shi, Mengliang Jiang, Munire Maimaiti, Yan Zhang, Yue Bai
School of Physics and Electronic Engineering, Xinjiang Normal University, Urumqi 830054, China.
Key points
From the paper's conclusion- This material has potential applications in temperature sensing and magnetic resonance imaging.
Abstract
Tm3+, Yb3+: GdxBi2-xWO6 series upconversion luminescent materials were synthesized via a solid-state method. Calculations and XRD analysis reveal that Gd3+ in the lattice exhibits both substitutional and interstitial doping. Compared with the NaYF4 matrix, the Bi2WO6 material doped with Gd3+ has a lower Debye temperature (392.45 K), and the maximum phonon energy is low; thus, the probability of nonradiative transitions decreases. SEM images and EDS results reveal that the powder particle size ranges from 0.5 to 3 μm and that the elements are evenly distributed on the surface. The diffuse reflectance absorption spectra indicate that moderate Tm3+, Yb3+ and Gd3+ doping shifts the absorption band of the material towards longer wavelengths and decreases the band gaps. Under 980 nm laser excitation and a Gd3+ doping concentration of x = 0.2, the emission intensities of Tm3+ at 476 nm, 683 nm, 703 nm, and 804 nm increase by 1.8, 1.24, 1.35, and 81.9 times, respectively. Calculations reveal that these emissions in the range of 450 to 850 nm originate from three-photon or two-photon absorption. Gd3+ codoping can prolong the lifetime of the Tm3+ energy levels. When this sample was excited at 980 nm (518 mW), the temperature was characterized by FIR703nm/476nm from 298 K to 573 K, and the obtained maximum relative sensitivity was 3.4907 K-1 (298 K). The minimum temperature resolution was 0.0083 K (298 K). Compared with that of the undoped Gd3+ sample, the temperature sensitivity of the Gd3+-codoped sample increased by 92.35 times. Under an external magnetic field of 20 kOe and a temperature of 300 K, the magnetization of the sample doped with Gd3+ increased fourfold to 0.08174 emu/g. This material has potential applications in temperature sensing and magnetic resonance imaging.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Temperature Dependent Upconversion Luminescence in Er³⁺ /Yb³⁺ Codoped BaY 0.67 Mo 0.33 O₃ Double Perovskite Phosphor for Optical ThermometryACS Applied Optical Materials · 2026
- Dual-mode luminescence, high-sensitivity optical thermometry and latent fingerprint visualization of Er3+-activated La2WO6 phosphors.Spectrochimica acta. Part A, Molecular and biomolecular spectroscopy · 2026
- Yb/Er Co‐Doped Double Perovskite Titanate Phosphors: Harnessing Upconversion for Advanced Optical Thermometry and NIR‐Triggered Green LEDsAdvanced Optical Materials · 2026
- Yb³⁺ Sensitized Er³⁺ Upconversion Phosphors for Noninvasive Luminescence‐Based Optical ThermometryJournal of the American Ceramic Society · 2026
- Enhancing sensitivity and detection range of Ca2GdZr2Al3O12:Bi3+,Tb3+ fluorescent thermometer via multi-excitation pathways and anti-thermal quenching.Spectrochimica acta. Part A, Molecular and biomolecular spectroscopy · 2026
- Non-interfering dual-mode luminescence with persistent emission under UV excitation and upconversion thermometry under NIR excitation in Ca3Ga4O9:Pr3+,Er3+,Zn2.Nanoscale · 2026