From the paper's conclusion- This study employed potassium hydroxide (KOH) to modify biochar derived from bamboo powder waste, activating it at different temperatures (700 °C, 800 °C, and 900 °C) to yield samples designated KBC-700, KBC-800, and KBC-900, respectively.
Abstract
Bamboo powder waste generated from bamboo processing serves as an ideal feedstock for biochar (BC). This study employed potassium hydroxide (KOH) to modify biochar derived from bamboo powder waste, activating it at different temperatures (700 °C, 800 °C, and 900 °C) to yield samples designated KBC-700, KBC-800, and KBC-900, respectively. The physicochemical properties and pore structures of the modified biochar were characterized using SEM, specific surface area and pore size analysis, FT-IR, Raman spectroscopy, XRD, and zeta potential measurements. The adsorption performance of the modified biochar toward PFOA was investigated using kinetic and thermodynamic models, examining the effects of the solution pH, adsorbent dosage, and temperature. Results indicate that KBC-900 exhibits a significantly enhanced specific surface area (up to 2924.7 m2 g−1), reduced surface oxygen-containing functional groups, increased carbon skeleton aromatization, and expanded mesoporous channels. Under initial conditions of pH = 3 and reaction temperature of 298 K, KBC-900 achieved a PFOA adsorption capacity of 366.7 mg g−1 with a removal efficiency of 91.67%. The adsorption process conformed to pseudo-first-order and pseudo-second-order kinetic models as well as the Freundlich model. The adsorption equilibrium was reached within 12 h, indicating multi-layer adsorption dominated by chemisorption on a heterogeneous surface. Thermodynamic parameters indicate the adsorption reaction is an exothermic process. After five cycles of regeneration, KBC-900 maintained a removal efficiency of 75.69%. This study provides an efficient and reliable solution for removing PFOA from water.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Tailoring Alfalfa-Derived Biochar via Pyrolysis Temperature for Enhanced Adsorption of Diverse Per- and Polyfluoroalkyl Substances in Water.ACS omega · 2026
- Adsorption of phosphates on a novel eggshell Ca-modified anaerobic sludge-based biochar: Adsorption performance and mechanismPLoS ONE · 2025
- Enhanced Adsorption of Bisphenol a on Lignin-Derived Biochars: Role of Thermal and Phosphoric Acid Activation in Surface Functionalization and MechanismPolymers · 2025
- Bamboo biomass-derived biochar for advanced water treatment: A comprehensive review of synthesis routes and perspectives on the removal of emerging contaminantsAdvances in Bamboo Science · 2026
- Overriding Surface Area Limitation: Mesopore-Driven Norfloxacin Adsorption on High-Temperature P-Doped Biochar.Materials (Basel, Switzerland) · 2026
- Deciphering Physicochemical Principles Guiding PFAS Adsorption and Thermal Degradation on Regenerable Waste-Derived BiocharEnvironmental Science & Technology · 2026