Resistance-Ratio Requirement of Memristive Processing-in-Memory Wafer Defect Classifiers: A Simulation Study with Four Representative Devices
Jeongwoo Choi, Hunhee Jeong, Mincheol Yoon, Soo-Whang Baek, Jonghwan Lee
Key points
From the paper's conclusion- Here, we compare four representative memristive devices (Pt/HfOx/Ti, Ferroelectric, Metallic Nanowire, and TaOx/Ta) whose low- and high-resistance states are taken from published VTEAM fits to measured devices, whereas their numbers of levels, variations, and fault rates are assumed.
Abstract
Classifying wafer map defects directly inside inspection equipment requires hardware that is fast and low-power, which makes memristor-based Processing-in-Memory (PIM) an attractive implementation of convolutional neural network (CNN) classifiers. A memristive classifier, however, is only as accurate as its devices allow: finite conductance levels, device-to-device variation, and stuck-at faults distort the stored weights, and what a device must provide for wafer defect classification to remain accurate has not been quantified. Here, we compare four representative memristive devices (Pt/HfOx/Ti, Ferroelectric, Metallic Nanowire, and TaOx/Ta) whose low- and high-resistance states are taken from published VTEAM fits to measured devices, whereas their numbers of levels, variations, and fault rates are assumed. We mapped the same CNN architecture onto each device’s crossbars with MemTorch and applied all three non-idealities together. On the Mixed Type and WM-811K datasets, the four devices differed by less than 0.01 in Macro F1 without non-idealities but separated with them. Metallic Nanowire collapsed (resistance ratio ρ = Roff/Ron ≈ 2; Mixed Type: Macro F1 0.973 → 0.109), whereas Ferroelectric (333×) and TaOx/Ta (146×) retained the highest F1-scores (two-dataset mean ΔF1 = −14.33% and −16.35%), with no significant difference detected between them. Under a common non-ideality profile, the three devices with ρ ≥ 25 showed no significant differences, and a controlled experiment that varied only ρ showed that a low ratio alone causes the collapse and that the loss saturates at ρ ≈ 10 on WM-811K and between 25 and 50 on Mixed Type. A fault-mitigation baseline changed neither the collapse at ρ = 2 nor the device ordering, and with wire resistance the devices with Ron ≤ 100 Ω failed. Within the simulated conditions, the results give a quantitative device requirement for memristive PIM defect classifiers: a resistance ratio of at least about 10, preferably 50–100, beyond which the stuck-at faults, not the ratio, dominate the remaining loss, and, with wire resistance, an on-resistance of about 1 kΩ or more.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Large-scale crossbar arrays based on three-terminal MoS2 memtransistorsNature Communications · 2025
- Hardware-Aware Ternary Neural Networks with Accuracy Recovery on Two-State Silicon Nanowire Memristive CrossbarsTechnologies · 2026
- Investigation on the Impact of Memristive Device Variability on Uncoupled Memristive Cellular Nonlinear NetworksAdvanced Electronic Materials · 2026
- TERNARY NEURAL NETWORK WITH SPARSE WEIGHT OPTIMIZATION FOR ENERGY-EFFICIENT MEMRISTOR CROSSBAR DEPLOYMENT WITH DEFECT TOLERANCEKufa Journal of Engineering · 2026
- Electrode area precision and odd-state quantization failure in neuromorphic memristive synapsesApplied Physics Letters · 2026
- High-Performance Conductive Bridging Memristor via van der Waals Interface Engineering for Neuromorphic Computing.Small (Weinheim an der Bergstrasse, Germany) · 2026