Influence of Post-Weld Heat Treatments on the Hydrogen Embrittlement Susceptibility of API 5L X52N Pipeline Steel Welded Joints

Unai De Francisco Vargas, Nora Guenaga Gomez, Nevena Vaskova Marinova, Pablo Benguria Uribe

Key points

From the paper's conclusion
  • This work evaluates the influence of post-weld heat treatments (PWHT) on the hydrogen embrittlement (HE) susceptibility of girth-welded API 5L X52N pipeline steels.

Abstract

This work evaluates the influence of post-weld heat treatments (PWHT) on the hydrogen embrittlement (HE) susceptibility of girth-welded API 5L X52N pipeline steels. Four conditions were analyzed: as-welded, two stress-relief treatments (HT1 at 635.1 °C and HT3 at 593.5 °C), and a normalizing treatment (HT2 at 911.4 °C). Mechanical characterization was performed via Slow Strain Rate Tests (SSRT) in high-pressure hydrogen (160 bar) and air. Normalizing (HT2) homogenized the joint microstructure and increased plastic elongation in air and hydrogen; however, it produced the lowest reduction-of-area retention among the cross-weld conditions (HEIRA = 0.57), indicating greater hydrogen sensitivity during localized final fracture, while its plastic-elongation retention remained comparable to the as-welded condition. Among stress-relief treatments, HT1 showed the most favorable ductility retention in the filler metal, although this observation rests on a single FM-fractured specimen per condition and is not statistically conclusive. Fractographic analysis revealed a transition from ductile dimples in air to mixed-mode fracture in hydrogen, characterized by transgranular quasi-cleavage. The study suggests that acicular ferrite in the filler metal offers greater resistance to hydrogen-induced crack propagation than the equiaxed polygonal-ferrite microstructure produced by normalizing.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers