Key points
From the paper's conclusion- The results indicated that through-wall microstructural banding originated from pearlite bands associated with C and Mn segregation during piercing and rolling.
Abstract
An ultra-low-Mn steel (MS) incorporating multiple alloying additions was designed for seamless pipes used in deepwater oil and gas transportation to eliminate through-wall microstructural banding and optimize the strength–toughness balance. Using a conventional pipeline steel (BS) as a reference, the effects of tempering temperature on the microstructure and mechanical properties of both steels were systematically investigated over 600–700 °C. The evolution of microstructural banding and the strengthening mechanisms were examined using optical microscopy, scanning electron microscopy, electron backscatter diffraction, electron probe microanalysis, transmission electron microscopy, and physicochemical phase analysis. The results indicated that through-wall microstructural banding originated from pearlite bands associated with C and Mn segregation during piercing and rolling. These bands persisted through subsequent heat treatment and could promote local hydrogen accumulation, thereby increasing susceptibility to hydrogen-induced cracking (HIC). Substantially reducing the Mn content while increasing the combined contents of Cr, Ni, and Mo and the microalloying additions of Nb, V, and Ti, together with appropriate heat treatment, reduced microstructural banding and produced a fine, uniform microstructure throughout the pipe wall. MS exhibited greater strength–toughness balance than BS across the entire tempering temperature range, with the optimum strength–toughness balance achieved at 660–680 °C. The favorable strength–toughness balance of MS was attributed to the combined effects of microstructural homogenization, dislocation recovery, grain-boundary evolution, and strengthening by nanoscale compound (Mo, Nb, Ti, V)C precipitates during tempering. The highest fraction of fine, dispersed precipitates was obtained at 660 °C, effectively compensating for recovery-induced matrix softening and maintaining a high strength level.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Effect of tempering temperature on hydrogen embrittlement of X60 pipeline steelInternational Journal of Hydrogen Energy · 2025
- Tailored heat treatments to characterise the fracture resistance of critical weld regions in hydrogen transmission pipelinesInternational Journal of Hydrogen Energy · 2025
- Hydrogen Embrittlement Resistance of an Austempered Martensite/Bainite Dual-Phase Steel.Materials (Basel, Switzerland) · 2026
- Investigation of Welded Joints of Pipelines from an Existing Gas Transmission Network Exposed to Hydrogen—Part II: Some Aspects of the Microstructural Mechanisms of Hydrogen-Assisted Damage and FractureMetals · 2026
- Study of the Resistance of Low-Alloy Pipe Steels to Hydrogen-Induced CrackingJournal of Manufacturing and Materials Processing · 2026
- The Effect of Cu-Rich Nano-Precipitation on Hydrogen Embrittlement Performance in a Cu-Bearing Ultra-Low Carbon Steel.Materials (Basel, Switzerland) · 2026