Study on Residual Stress and Deformation Control in Argon Arc Repair of WE43A Magnesium Alloy
Faming Shen, Ziyin Zhang, Xin Zheng, Liyan Zhang, Kai Zhou, Yonghua Han
Key points
From the paper's conclusion- This study provides a numerical theoretical reference for process optimization of low-stress, small-deformation argon-arc repair welding of WE43A magnesium-alloy casing castings, while it should be noted that mechanical-field outputs have not been independently validated by experimental measurements.
Abstract
To address the problems of high residual stress, high cracking susceptibility, and deformation in argon arc repair welding of casting defects in WE43A rare-earth magnesium alloy aero-engine casing castings, a thermo-mechanical coupled finite element model considering the high-temperature properties of the material was established. A double ellipsoid heat source was used to simulate the heat input of argon arc welding, and the effects of the repair welding path, preheating before welding, post-weld heat treatment, and number of repair holes on the residual stress and deformation of repaired components were systematically investigated. The results show that the repair welding path significantly affects residual stress. The peak von Mises equivalent residual stress under a parallel repair welding path reaches 248 MPa, suggesting a relatively high potential cracking risk based on an empirical reference threshold. Under a circular repair welding path, the peak stress decreases to 199.4 MPa, effectively alleviating stress concentration. Increasing the preheating temperature can simultaneously reduce residual stress and welding warpage deformation. Compared with the 150 °C condition, preheating at 350 °C reduces warpage deformation by up to 45%. The residual stress release effect of post-weld heat treatment is enhanced with increasing temperature. Post-weld heat treatment at 450 °C for 1 h can reduce the peak residual stress by nearly half, but low- and medium-temperature post-weld heat treatments have a limited inhibiting effect on the macroscopic deformation of the component. Under the condition of side-hole repair welding on the curved surface of the casing, double-hole repair welding slightly reduces the peak stress and deformation compared with single-hole repair welding, but expands the stress influence range. This study provides a numerical theoretical reference for process optimization of low-stress, small-deformation argon-arc repair welding of WE43A magnesium-alloy casing castings, while it should be noted that mechanical-field outputs have not been independently validated by experimental measurements.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Microstructural Modification and Strengthening Mechanisms in a ZM6 Magnesium Alloy Joint Processed by Ultrasonic-Assisted TIG Welding with Pre-Weld Heat TreatmentCrystals · 2026
- Achieving defect-free repair in ZM6 magnesium alloy through cold metal transfer welding combined with preheatingJournal of Materials Research and Technology · 2026
- The role of in-situ phase transformation behavior on mechanical heterogeneity in Mg-7Gd-3Y-1Zn-0.5Zr alloy fabricated by wire-arc additive manufacturingJournal of Magnesium and Alloys · 2025
- Triggering ultrastrong age‐hardening response of laser‐powder bed‐fused WE43 alloy via solid solution temperature designRare Metals · 2025
- The effect of heat treatment on microstructure and mechanical properties of a high-strength Al–Mg–Mn-Sc-Ti alloy fabricated by wire arc directed energy depositionJournal of Materials Research and Technology · 2025
- Recent progress in wire arc additive manufacturing of magnesium alloysJournal of Magnesium and Alloys · 2026