Metals

Ethylene Carbonate Modulates Copper(I) Coordination in Copper Electrodeposition from DMI–AlCl3–Cu2O Electrolytes

Pingping Guan, Yongqi Liu, Shuo Peng, Zhiliang Wang, Xiaoming Yang, Xingxing Yu

Key points

From the paper's conclusion
  • Ethylene carbonate (EC) was added at 4.6–16.1 mol% to an 86.5DMI–9.6AlCl3–3.9Cu2O electrolyte (DMI: 1,3-dimethyl-2-imidazolidinone), and copper was electrodeposited at 333 K.

Abstract

Aqueous cyanide, sulphate, and acid copper baths are toxic, couple galvanically with aluminium and zinc substrates, or occlude hydrogen. Organic-solvent electrolytes avoid these routes, but their neutral additives remain little studied. Ethylene carbonate (EC) was added at 4.6–16.1 mol% to an 86.5DMI–9.6AlCl3–3.9Cu2O electrolyte (DMI: 1,3-dimethyl-2-imidazolidinone), and copper was electrodeposited at 333 K. Raman spectroscopy, conductivity, viscosity, voltammetry, electron microscopy, optical surface imaging, and density functional theory on Cu13(111) linked the solution structure to the deposit. EC raised the conductivity (323–363 K) to 4.19–8.23 mS cm−1 and the viscosity (323–373 K) to 6.3–13.2 mPa s, and shifted the onset potential from −0.4 to −0.85 V and the cathodic peak from −1.35 to −1.77 V. At −1.4 V, raising EC from 4.6 to 12.6 mol% reduced the apparent size of the surface features from 35 to 15 μm and peak-to-valley roughness from 1.7 to 0.9 μm, with smoothness ceasing to improve at 16.1 mol%. On Cu13(111), DMI adsorbed at −98.1 to −126.9 kJ mol−1 and 0.34–0.42 e, and EC at −38.7 to −62.4 kJ mol−1 and 0.11–0.19 e. Complexation energies fell from −79.7 to −57.4 kJ mol−1, so EC binds weakly in the first coordination shell. EC thus acts as a coordination modifier, not an adsorption inhibitor.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers

Ethylene Carbonate Modulates Copper(I) Coordination in Copper Electrodeposition from DMI–AlCl3–Cu2O Electrolytes — Science Skim