Protection of Magnesium Against Corrosion by Hot Vapors of Stearic Acid
Victoriia Luchkina, Ilia Kuznetsov, Nikolay Andreev, Da-Quan Zhang, Andrei Luchkin
Key points
From the paper's conclusion- The protective effect of stearic acid (SA) hot vapors on commercially pure magnesium (Mg90) was studied using accelerated corrosion tests under periodic moisture condensation, potentiodynamic polarization, electrochemical impedance spectroscopy, ellipsometry, and Kelvin probe force microscopy.
Abstract
The protective effect of stearic acid (SA) hot vapors on commercially pure magnesium (Mg90) was studied using accelerated corrosion tests under periodic moisture condensation, potentiodynamic polarization, electrochemical impedance spectroscopy, ellipsometry, and Kelvin probe force microscopy. The aim of this work was to establish the optimal conditions for the chamber treatment of Mg90 in hot SA vapor and to elucidate the mechanism of the protective effect, including its evolution during subsequent air exposure. Magnesium samples were treated in sealed chambers with SA vapor at 40–150 °C for 5–180 min and subsequently exposed to air for 0.5–144 h. The optimal conditions were found to be 140 °C and 15 min, under which nanoscale films up to 15 nm thick were formed. Longer treatment led to the condensation of excess SA and the formation of visible films with a lower protective effect. The adsorption layers freshly formed under optimal conditions did not provide substantial protection; their protective properties developed during subsequent air exposure and reached a maximum after 24–72 h. The time to the onset of corrosion increased from 0.5 h (untreated magnesium) to 52 h. The novelty of this work lies in the first systematic assessment of hot SA vapor as a chamber corrosion inhibitor for magnesium: the optimal treatment conditions were determined, the critical role of air exposure in the development of the protective properties was demonstrated, and a mixed inhibition mechanism with a predominant blocking contribution was established.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Frequency-Controlled AC-MAO Coatings with Ca, P, and Se on Magnesium: Toward Tailored Surfaces for Biodegradable ImplantsMaterials · 2025
- Adsorption, kinetic, thermodynamic, thermal stability, and RSM optimization studies of Mitragyna speciosa as a green corrosion inhibitor for API 5 L X65 steel in aggressive oil and gas well treatment fluidsChemical Thermodynamics and Thermal Analysis · 2026
- Insights of stearic acid/polypyrrole superhydrophobic coating on controlling corrosion, antibacterial and cytocompatibility of biodegradable Mg alloy and its implication on fracture fixationJournal of Magnesium and Alloys · 2025
- Eco-friendly corrosion inhibitors (combination of Macaranga gigantea sap extract and maltodextrin) on mild steel in sulfuric acid mediaResults in Surfaces and Interfaces · 2026
- Hybrid PEO–hydrothermal–silane coating with synergistic Ce–8HQ inhibitor sealing for durable corrosion protection of AZ31 magnesium alloynpj Materials Degradation · 2026
- From protection to failure: Oxidation of pure Mg and rare-earth-enhanced Mg alloys at elevated temperatureJournal of Magnesium and Alloys · 2025