Corrosion Resistance of Zinc Flake Coatings: Effect of Flake Morphology and Lamellar Microstructure

Junbeom Park, Seonghun Woo, Inyoung Park, Beomsoo Kim, Jung-Pil Noh, Kyunghwang Lee, Youngjong Kim, JeongHyeon Yang

Key points

From the paper's conclusion
  • Larger flakes and a higher estimated end-member α were not accompanied by higher resistance; packing quality should be considered alongside flake size and thickness.

Abstract

Classical tortuosity models predict improved barrier performance with increasing flake aspect ratio α (lateral dimension/thickness), other factors being equal. Four coatings from zinc pigments milled for 30, 60, 90 and 120 min (AR-L, AR-ML, AR-MH and AR-H, respectively) were compared. Segment Anything Model segmentation of SEM images showed that longer milling increased the median projected area from 11.4 to 23.2 μm2 and decreased the mean circularity from 0.74 to 0.63, without a systematic change in the in-plane axis ratio; with focused ion beam (FIB) thicknesses, α was estimated at about 10 for AR-L and 17 for AR-H. In 3.5 wt.% NaCl, electrochemical impedance spectroscopy (two specimens per condition) gave AR-L about twice the mean low-frequency resistance of the other coatings, whose differences were within specimen scatter, and AR-L had the highest polarization resistance at all 24 measurements over 25 h (2.7–5.2 times the next highest; one specimen per condition). Limited FIB sections showed the most compact, continuous lamellae in AR-L, tilted and bridging flakes in AR-MH and locally disordered regions in AR-H. Larger flakes and a higher estimated end-member α were not accompanied by higher resistance; packing quality should be considered alongside flake size and thickness.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers