Metals

Effects of Al Substitution for Si on Lath Refinement, Retained Austenite Stability, and Strength–Ductility Balance in Carbide-Free Bainitic Steels

Hongliang Zhang, Zijia Qu, Dezhi Li, Jie Li, Xianming Zhao

Key points

From the paper's conclusion
  • Lath refinement and changes in RA stability affected yielding and strain hardening differently, with A08 achieving a favorable strength–ductility balance.

Abstract

Si and Al modify the microstructure and properties of carbide-free bainitic steels, but the effects of their relative proportions at a fixed nominal combined content require further clarification. Three steels containing a nominal total of 1.8 wt.% Si + Al were austenitized at 950 °C for 300 s and isothermally held at 350 °C for 1000 s. Dilatometry, microstructural characterization, X-ray diffraction, and tensile testing were used to investigate transformation behavior, microstructure, retained austenite (RA) stability, and mechanical properties. With increasing Al/Si ratio, the mean bainitic ferrite lath thickness decreased from 206.2 nm in A0 to 196.1 nm in A08 and 155.2 nm in A10. A10 exhibited a higher relative transformation rate during the early and intermediate stages. The estimated RA carbon content and proportion of film-like RA increased, while the cumulative fraction of RA transformed during tensile testing to fracture decreased from 65.3% to 29.2%. A08 sustained a high strain-hardening rate over a broad strain range, achieving an ultimate tensile strength of 1016.3 ± 15 MPa and an elongation after fracture of 26 ± 0.4%. A10 exhibited the highest yield strength of 741.3 ± 11 MPa. Lath refinement and changes in RA stability affected yielding and strain hardening differently, with A08 achieving a favorable strength–ductility balance.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers