  • This work deals with the effect of a graded tungsten addition on the hot tearing susceptibility of the hypoeutectic AlSi5Cu2Mg alloy.

Abstract

Hot tears are among the most serious casting defects and limit the applicability of Al-Si-Cu-Mg alloys in automotive castings. This work deals with the effect of a graded tungsten addition on the hot tearing susceptibility of the hypoeutectic AlSi5Cu2Mg alloy. Tungsten was introduced through an AlW5 master alloy in nominal additions of 0.05, 0.10 and 0.15 wt.%, corresponding to measured contents of 0.020, 0.044 and 0.075 wt.%. The susceptibility was evaluated using a five-arm restrained casting mould equipped with a load cell and a thermocouple, by three variants of the hot tearing index and by a qualitative evaluation of the load curve and its first derivative. The nominal 0.05 wt.% addition decreased all three indices into the minimal-to-low susceptibility category, whereas higher additions led to a renewed rise, and at 0.15 wt.% the values reached the level of the reference alloy. The qualitative evaluation confirmed this trend. Thermal analysis showed an increase in the liquidus temperature from 615 to 629 °C and a corresponding widening of the solidification interval. The favourable effect of the low addition is attributed to a possible grain refinement of the primary phase, whereas at higher contents the widened solidification interval prevails.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers