Degassing Window for Jet-Milled HPMS NdFeB Powder Recycled from Wind-Turbine Magnets: Hydrogen Desorption and Magnetic Recovery
Alba Berja, Laura Grau, Benjamin Podmiljsak, Spomenka Kobe, Carlo Burkhardt, Jose Francisco Fernández, Adrián Quesada
Key points
From the paper's conclusion- This study defines a phenomenological degassing window for HPMS jet-milled powder from end-of-life wind-turbine magnets by screening degassing temperature (650–900 °C), heating rate (1–3 °C/min), and dwell time (5–60 min) under vacuum.
Abstract
Hydrogen processing of magnetic scrap (HPMS) is a promising short-loop route for recycling end-of-life NdFeB permanent magnets; however, the resulting hydrogenated powder requires vacuum degassing before reuse. This study defines a phenomenological degassing window for HPMS jet-milled powder from end-of-life wind-turbine magnets by screening degassing temperature (650–900 °C), heating rate (1–3 °C/min), and dwell time (5–60 min) under vacuum. Pressure–temperature desorption traces were deconvoluted into three Gaussian components (R2 = 0.999), associated with hydrogen release from the Nd2Fe14BHx matrix and NdH2.7/NdH2 grain boundary phases, and correlated with SEM-EDS microstructural analysis and magnetic properties (Hc, Mr, and M(1700 kA m−1)). Among the heating rates tested, 2 °C/min gave the most favorable combination of properties. Under this condition, the coercivity reached 434.1 kA/m after degassing at 900 °C, which we tentatively attribute to the recombination of α-Fe and Nd into Nd2Fe14B, while M(1700 kA m−1) peaked at 99.8 A·m2/kg at 880 °C. Coercivity recovery depends primarily on the peak degassing temperature rather than on the time spent above 800 °C. The oxygen content increased from 0.46 wt.% after HPMS to 0.59 wt.% after jet milling and 0.66 ± 0.06 wt.% after degassing at 900 °C, which makes oxygen control a key limitation of the route. The results reveal a trade-off between coercivity and M(1700 kA m−1) that can be tuned within a single degassing step, and a degassing window distinct from that established for powders intended for re-sintering. The suitability of the recovered powder for bonded magnets remains to be demonstrated.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Ball-Milling Processing of Hydrogenated NdFeB Powders from the Recycling of End-of-Life Magnets.Materials (Basel, Switzerland) · 2026
- A hydrothermal process for recycling SmCo5 permanent magnetsJournal of Magnetism and Magnetic Materials · 2026
- An Innovative Hydrometallurgical Process for the Recycling of Spent NdFeB Magnets: Process Optimization and AnalysisMinerals · 2026
- Hydrogen-induced degradation in sintered NdFeB magnets: A comprehensive study on microstructural evolution and multi-scale property deteriorationJournal of Materials Research and Technology · 2026
- Comparative study on the efficient pre‐treatment processing for rare earth elements recovery from magnet wasteMaterialwissenschaft und Werkstofftechnik · 2026
- The Viability of Sol–Gel Coatings for the Corrosion Protection of NdFeB Permanent MagnetsCorrosion and Materials Degradation · 2026