Effect of Pre-Corrosion on the Fatigue Behavior of 347H Austenitic Stainless Steel at Elevated Temperature
Hao Chen, Hai-Ying Lei, Xue-Jing Sun, Jian-Guo Gong, Yu-Hui Huang, Fu-Zhen Xuan
Key points
From the paper's conclusion- The pre-corrosion does not alter the cyclic hardening characteristic of 347H stainless steel but significantly reduces its fatigue life.
Abstract
The combined damage induced by the nitrate molten salt corrosion and cyclic loading at elevated temperatures is an important damage issue for the reliable operation of concentrated solar power (CSP) plants. In previous works, the effect of the molten salt pre-corrosion on the fatigue behavior of 347H stainless steel remains insufficiently understood. Based on this, the present work investigated the corrosion behavior of 347H stainless steel in nitrate molten salts at 565 °C, with particular attention to chloride impurities. The effects of pre-corrosion on cyclic deformation characteristics, fatigue life, and failure mechanisms were discussed. The results indicated that the oxide-scale growth follows approximately parabolic kinetics in chloride-free salt, whereas chloride-containing salt exhibits sub-parabolic growth with a lower kinetic exponent. Chloride addition produces a thicker and less stable oxide scale characterized by cracking, spallation, and chromium depletion. The pre-corrosion does not alter the cyclic hardening characteristic of 347H stainless steel but significantly reduces its fatigue life. The corrosion-induced damage morphology also changes the subsequent fatigue crack initiation behavior. The relatively uniform oxidation promotes crack initiation at the oxide layer-substrate interface, whereas chloride-induced scale degradation introduces more severe local damage and accelerates crack initiation and propagation.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Corrosion Behavior of Stainless Steels and Superalloys at 800°C and 900°C in an Oxidizing EnvironmentMaterials and Corrosion · 2026
- Cyclic deformation behavior and fatigue life prediction of 316H stainless steel under strain-controlled fatigueJournal of Materials Research and Technology · 2026
- Cyclic oxidation behavior and internal nitridation of GH4738 superalloy at 750–950 °CJournal of Materials Research and Technology · 2026
- Effect of thermal cycling and phase transformations on chemical life of ferritic stainless steelsCorrosion Science · 2026
- Combined Effects of Pre‐Strain and Sensitization on Corrosion Fatigue Behavior of Type 304 Stainless SteelFatigue & Fracture of Engineering Materials & Structures · 2026
- Type II hot corrosion of the polycrystalline nickel-based superalloy AD730 in presence of Na2SO4 and Na2SO4-MgSO4 depositsCorrosion Science · 2026