Effect of Hot Isostatic Pressing Temperature on Microstructure and Properties of TC21 Titanium Alloy
Haiyang Zhang, Chenyang Li, Jun Yin, Zhuan Qi, Ke Hua, Haifeng Wang, Weimin Liu
Key points
From the paper's conclusion- These results clarify the HIP-temperature-dependent microstructure–property relationship of PM-HIP TC21 alloy and provide guidance for optimizing HIP parameters of powder-metallurgy titanium alloys.
Abstract
Powder metallurgy combined with hot isostatic pressing (PM-HIP) enables the fabrication of near-net-shape titanium alloy components with near-theoretical density, yet the HIP temperature fundamentally determines the densification behavior, phase constitution and mechanical properties of the consolidated alloy. In this work, TC21 pre-alloyed powder is consolidated by HIP at 890 °C, 920 °C, 950 °C, 980 °C and 1010 °C under 140 MPa for 3 h, followed by furnace cooling, and all the as-HIPed compacts are subsequently subjected to a two-step heat treatment (900 °C/1 h/air cooling + 590 °C/4 h/air cooling). The microstructure in both the as-HIPed and heat-treated states is characterized by SEM (scanning electron microscope), XRD (X-ray Diffraction), EBSD (Electron Back Scatter Diffraction) and TEM (transmission electron microscope), and the room-temperature tensile properties are evaluated. The results show that increasing the HIP temperature coarsens the primary α (αp) and secondary α (αs) phases while promoting the precipitation of αs in the β matrix. The competition between the precipitation strengthening of αs and microstructural coarsening governs the strength–ductility balance, and the alloy HIPed at 950 °C attains the optimum properties after heat treatment, with an ultimate tensile strength of 1259.5 ± 3.63 MPa, a yield strength of 1195.5 ± 3.5 MPa, an elongation to fracture of 13 ± 2.82% and a reduction of area of 35.5 ± 2.12%. The superior performance is attributed to the high volume fraction of fine αs lamellae, which provides pronounced precipitation strengthening, together with an appropriate amount of αp phase, which preserves strain-hardening capacity and ductility. These results clarify the HIP-temperature-dependent microstructure–property relationship of PM-HIP TC21 alloy and provide guidance for optimizing HIP parameters of powder-metallurgy titanium alloys.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Toughness Effect and Strengthening Mechanisms of Manifold Microstructures on Hot Isostatic Pressing Ti55541 Metastable β-Titanium AlloyMetals · 2026
- Achieving Strength–Ductility Synergy in a Near‐α Powder Metallurgy Titanium Alloy via Deformation‐Induced Nanoscale β PrecipitationRare Metals · 2026
- Metallurgical Defects and Tensile Properties of a High Nb–TiAl Alloy Fabricated by Hot Isostatic Pressing of Prealloyed PowderAdvanced Engineering Materials · 2025
- Microstructure evolution and mechanical performance of diffusion-bonded Ti-6.5Al–2Zr–1Mo–1V alloy components fabricated by preform hot isostatic pressingJournal of Materials Research and Technology · 2025
- Evaluation of Microstructure and Mechanical Behavior of Ti p /AZ91 Composites Produced by Hot Press SinteringMaterials Research Express · 2026
- Effects of quasi-β phase forging plus duplex ageing process on microstructure evolution and mechanical properties of TC18 alloyMaterials Today Communications · 2026