Conversion of Li3PO4 Derived from LiFePO4 Cathode Manufacturing Byproducts to Li2CO3 via CaCO3-Assisted CO2 Thermal Treatment

Do-Hee Kim, Jei-Pil Wang

Key points

From the paper's conclusion
  • These results demonstrate the feasibility of recovering lithium from LFP cathode manufacturing byproducts through controlled phase conversion and water-based separation, while also highlighting the need to improve Stage I lithium recovery and to consider the thermal-energy demand associated with solution concentration and drying during future process development.

Abstract

A sequential lithium-recovery process combining hydrogen reduction, water leaching, CaCO3-assisted thermal conversion under a CO2 atmosphere, and a second water-leaching step was investigated using an LFP cathode manufacturing byproduct as the starting material. Hydrogen reduction was first employed to decompose LiFePO4 and redistribute lithium into a Li3PO4-containing phase while Fe and P were predominantly incorporated into Fe-rich phosphide phases. Among the investigated conditions, treatment at 900 °C for 3 h resulted in the disappearance of detectable LiFePO4 peaks and the formation of Li3PO4 and Fe2P as the predominant crystalline phases. The reduced product was subsequently subjected to water leaching, and a solid-to-liquid ratio of 1:100 with a leaching time of 5 h yielded a Li3PO4-rich intermediate with a lithium recovery of 45.06% and a Li content of 17.43 wt.%. The recovered intermediate was then mixed with CaCO3 and thermally treated under a CO2 atmosphere to convert lithium phosphate into lithium carbonate while phosphorus was transferred into a Ca–P-rich phase. The most favorable phase-conversion behavior was obtained at 900 °C using a Li3PO4-to-CaCO3 weight ratio of 1:1 and a holding time of 2 h, where Li2CO3 and Ca2P2O7 were identified as the predominant crystalline products. Subsequent water leaching separated the Li-containing carbonate fraction from the water-insoluble Ca2P2O7-rich residue. A maximum lithium recovery of 93.59% was obtained at a solid-to-liquid ratio of 1:50 in the solid-to-liquid-ratio experiments, while the leaching-time experiments showed a lithium recovery of 92.54% after 5 h under the same solid-to-liquid ratio. XRD analysis of the final recovered product identified Li2CO3 as the predominant crystalline phase. Based on the selected conditions for Stage I and Stage II, the cumulative lithium recovery from the initial LFP feed to the final Li2CO3-rich product was approximately 41.70%, indicating that the first water-leaching and Li3PO4-intermediate recovery step was the principal limitation of the overall process. These results demonstrate the feasibility of recovering lithium from LFP cathode manufacturing byproducts through controlled phase conversion and water-based separation, while also highlighting the need to improve Stage I lithium recovery and to consider the thermal-energy demand associated with solution concentration and drying during future process development.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers