Effects of Magnesium on the Microstructure of Hypereutectic Al–20Si Alloys
Liang Hu, Hui Zhao, Guanglin Zhu, Wenqi Han, Fengling Zhang, Xiaohao Yi, Qinru Tang, Wenhuan Shen
Shenyang Ligong University · Northeastern University
Key points
From the paper's conclusion- A detailed analysis of the effects of magnesium on the microstructure of hypereutectic Al–20Si alloys is provided in this study.
Abstract
A detailed analysis of the effects of magnesium on the microstructure of hypereutectic Al–20Si alloys is provided in this study. Experimental results show that the addition of Mg significantly refines the primary silicon phase relative to the unmodified Al–20Si alloy, transforming its morphology from a complex form to a singular plate-like structure. Notably, for the first time, equiaxed aluminum grains appear in the aluminum matrix under conventional solidification conditions. The generation of these grains is closely related to the quenching effect caused by rapid cooling during metal mold casting, which promotes the generation of equiaxed aluminum grains within tightly constrained temporal and spatial parameters. The Al–Si eutectic structure exhibits a regular lamellar morphology, with an average eutectic silicon spacing of 930.97 nm. The phase analysis shows that the alloy mainly consists of Al, Si, and Mg2Si phases after the addition of Mg. With the increase in Mg concentration, the diffraction peaks for Al(200) and Si(220) first shift to lower angles and then move to higher angles, along with significant peak broadening. Ambient temperature mechanical testing indicates that tensile strength first increases with increasing Mg concentration, then declines, with the highest tensile strength of 235.1 MPa at 3 wt.% Mg in the Al–20Si alloy. The fracture mechanism of the testing specimens changes from cleavage fracture to ductile fracture. Microhardness testing indicates a continuous increase in the hardness of the aluminum matrix with rising Mg concentration; the hardness of primary silicon declines first and then increases, whereas the hardness of the eutectic structure exhibits a first increase followed by a decline.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Experimental investigation of compressive failure behaviour and image-based micromechanical analysis of hypereutectic Al–Mg2Si compositesModelling and Simulation in Materials Science and Engineering · 2026
- Unraveling the Distinct Roles of Al and Ca in Microstructure Evolution and Tensile Response of Extruded Mg–Al–Ca AlloysMaterials · 2026
- Effects of addition of Mn on microstructure, mechanical properties and corrosion behavior of T6-treated Al-Si-Mg alloysTransactions of Nonferrous Metals Society of China · 2026
- Elimination of stretcher strain marks in high-Mg Al-Mg alloys: deformation behavior and microstructural insights in H16 temperMaterials Science and Engineering A · 2025
- Microstructure and mechanical property of large-diameter and low-alloyed Mg-Mn-Ca-Ce-Al alloyMetals Advances · 2026
- Grain refinement and mechanical enhancement in high-speed-extruded Mg–5Bi–3Al Alloy via Si microalloyingJournal of Materials Research and Technology · 2025