From the paper's conclusion- This study compared aluminium-sol- and silica-sol-derived SiC membranes fabricated in air at 1300 °C with sol additions of 10–40 wt.%, focusing on pore structure, mechanical strength, mine-water filtration, fouling behaviour, and alkaline oxidative cleaning.
Abstract
Low-temperature fabrication of porous silicon carbide (SiC) ceramic membranes using secondary bonding phases offers an alternative to conventional high-temperature sintering. This study compared aluminium-sol- and silica-sol-derived SiC membranes fabricated in air at 1300 °C with sol additions of 10-40 wt.%, focusing on pore structure, mechanical strength, mine-water filtration, fouling behaviour, and alkaline oxidative cleaning. X-ray diffraction revealed weak features potentially associated with mullite formation in the aluminium-sol membranes, while SiO2-related phases were observed in the silica-sol membranes. Increasing sol content reduced porosity, pore diameter, and permeate flux while improving flexural strength. SiC-30%Al-sol provided a favourable performance balance, achieving a flexural strength of 25.2 MPa, a permeate flux of approximately 230 L m-2 h-1 after 40 min of mine-water filtration, and a final permeate turbidity of approximately 0.3 NTU. For SiC-30%Al-sol, the cake-filtration model provided the best fit over the 5-20 min interval, without establishing the dominant fouling mechanism. Following a single NaOH/NaClO cleaning cycle, SiC-30%Al-sol exhibited 90.4% flux recovery and 15.1% flexural-strength loss. Aluminium-sol membranes generally showed smaller strength losses and surface-roughness changes than silica-sol membranes under the tested conditions. These findings highlight the influence of bonding-phase chemistry on membrane performance, although repeated cleaning and post-cleaning pore-structure measurements are needed to establish long-term durability.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Microstructure and Mechanical Properties of Electrospun SiC / SiO 2 Fibrous Membranes Tuned by Nano‐ SiO 2 DopingJournal of Applied Polymer Science · 2026
- Architectural design of ceramic membranes to decouple mechanical strength and gas permeance for energy and environmental sustainabilityGreen Energy & Environment · 2026
- Review of Sustainable Ceramic Membranes for Wastewater Treatment: Raw Materials, Fabrication, and ApplicationsSVU-International Journal of Engineering Sciences and Applications · 2026
- A Novel Binder-Assisted Atmospheric Sintering Route for Silicon Carbide (SiC) Production.ACS omega · 2026
- Eco-Friendly Ceramic Membranes from Natural Clay and Almond Shell Waste for the Removal of Dyes and Drugs from WastewaterMembranes · 2026
- Slurry Carbon–Driven Pore Evolution, Infiltration, and Mechanical Properties of Continuous Carbon Fiber‐Reinforced Silicon Carbide Composites Prepared by Slurry Impregnation Combined With Reaction Melt InfiltrationJournal of the American Ceramic Society · 2026