Study on the Effect of Cu(Y/Gd) Addition Conditions on the Magnetic Properties and Microstructure of Sm(Fe0.8Co0.2)11Ti Alloy
Zhijie Xu, Sujuan Wang, Shuwei Zhong, Sajjad Ur Rehman, Chen Jiang, Xiao Gao, Munan Yang, Jiajie Li
Key points
From the paper's conclusion- The intrinsic relationship between the microstructure evolution and magnetic properties of the magnets with different element-addition methods was systematically revealed.
Abstract
ThMn12-type SmFe12-based compounds exhibit outstanding intrinsic magnetic properties and hold significant promise as low-cost, high-performance permanent magnets. However, the development of high-performance bulk magnets remains highly challenging due to the intrinsic lattice mismatch and the absence of continuous grain-boundary phases in the ThMn12-type crystal structure. In this study, Cu, CuY, and CuGd were introduced into the Sm(Fe0.8Co0.2)11Ti base alloy via two different element-addition methods, namely addition by melting and grain-boundary addition. SmFe12-based nanocrystalline magnets were prepared by spark plasma sintering (SPS). The intrinsic relationship between the microstructure evolution and magnetic properties of the magnets with different element-addition methods was systematically revealed. The experimental results show that Cu is more suitable for entering the magnet by grain-boundary addition, forming a continuous non-ferromagnetic Sm-Fe-Cu grain-boundary phase, inhibiting the formation of the SmFe2 phase, and effectively improving the stability and coercivity of the main phase. In this case, the best magnetic properties are obtained: the remanence is 6.699 kGs, the coercivity is 4.405 kOe, and the maximum magnetic energy product is 7.029 MGOe. The Cu element added by melting may lead to the abnormal growth of the grain size of the magnet and may deteriorate the performance of the magnet. The Y and Gd elements act as high-melting-point elements in the magnet to inhibit the grain growth of the magnet. This effect is more obvious in the magnet added by melting, and the obtained magnet structure is more uniform, and the squareness is higher (Hk/Hcj = 32.9%).
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- The effects of CeFe2 phase distribution and magnetic transition on the magnetic behavior of hot-deformed Ce16Fe76Cu2B6 magnetApplied Physics Letters · 2026
- Identifying grain boundary and intragranular pinning centres in Sm2(Co,Fe,Cu,Zr)17 permanent magnets to guide performance optimisationNature Communications · 2025
- Recent Progress in High‐Performance Sm₂ Co₁₇ ‐Type MagnetsAdvanced Functional Materials · 2026
- Cu-assisted Tb in situ grain boundary diffusion Nd-Fe-B magnet by high pressure torsion: magnetic properties and microstructureJournal of Materials Research and Technology · 2026
- Synergistic Enhancement of Tb Diffusion Efficiency in Nd-Ce-Fe-B-Sintered Magnets by Ferromagnetic Elements of Fe and NiMagnetochemistry · 2026
- Research on the microstructure evolution and segregation characteristics of Sm25Co48.5Fe19Cu4.8Zr2.7 alloy with different cooling rates during directional solidificationJournal of Materials Research and Technology · 2026