Formation and Evolution of Inclusions During the Refining Process of High-Cr Martensitic Stainless Steel
Shiheng Liang, Yuanxiang Ling, Xianxiang Su, Jiaji Wang, Wei Liu, Bo Song
Key points
From the paper's conclusion- These findings provide an industrial basis for optimizing inclusion control and improving steel cleanliness in L80-13Cr steel.
Abstract
L80-13Cr is a high-Cr martensitic stainless steel widely used for oil-well casing, yet the evolution of non-metallic inclusions throughout industrial LF-VD refining remains insufficiently understood. This study systematically investigated inclusion evolution during industrial ladle furnace (LF) and vacuum degassing (VD) refining by combining chemical analyses of molten steel and refining slag, automated inclusion analysis, scanning electron microscopy and energy-dispersive spectroscopy (SEM/EDS) characterization, and thermodynamic phase-diagram analysis. During LF refining, alloy composition adjustment, deoxidation, and desulfurization were accompanied by compositional changes in Ca-Mg-Al-O- and CaS-containing inclusions toward MgO·Al2O3- and Ca-containing aluminate inclusions. During VD refining, total oxygen (T[O]) and total nitrogen (T[N]) decreased from 17 × 10−6 and 290 × 10−6 to 11 × 10−6 and 145 × 10−6, respectively. Following Ca-Si treatment, the inclusion population shifted toward Ca-containing aluminates and Ca-Mg-Al-O inclusions, accompanied by the formation of CaS-containing composite inclusions. Subsequent soft blowing reduced the population of coarse inclusions (>5 μm), while the residual inclusion population shifted toward smaller sizes. Thermodynamic analysis showed that the average inclusion compositions shifted toward the CaO-rich and subsequently CaS-rich regions but remained outside the liquid-phase region at 1600 °C, indicating incomplete modification of the average inclusion population. By combining stage-resolved industrial observations with quantitative inclusion statistics and thermodynamic analysis, this study clarifies the continuous evolution of inclusions throughout LF-VD refining. These findings provide an industrial basis for optimizing inclusion control and improving steel cleanliness in L80-13Cr steel.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Evolution of non-metallic inclusions in an Al-killed, Ca-treated, low-S steel during industrial secondary refiningScientific Reports · 2026
- Influence of La–Ce Rare‐Earth Addition Routes on Elemental Homogeneity and Inclusion Modification in H13 Hot‐Work Tool Steelsteel research international · 2026
- Study on the effect of composite rare earths on the inclusion evolution in Al-containing steelHigh Temperature Materials and Processes · 2026
- Effect of rare-earth modified inclusions on the initiation of marine localized corrosion in high-strength low-alloy steelJournal of Materials Research and Technology · 2026
- Influence of La Addition on the Precipitation Behavior of Ti‐Containing Inclusions During Solidification of High‐Titanium Wear‐Resistant Steelsteel research international · 2026
- Synergistic Inclusion Modification in Steel Using Calcium, Magnesium, Rare Earths, and Hybrid Treatments: A Reviewsteel research international · 2025