Materials

Effect of Bilayer Repetition Number on the Microstructure and Scratch Failure Behavior of TiN/Rh Multilayer Coatings

Haoxuan Zhang, Chenjing Qiang, Xuanze Qin, Haomin Hou, Zongbin Li, Bo Yang

Key points

From the paper's conclusion
  • These findings demonstrate that increasing the number of ceramic/metal interfaces does not necessarily improve scratch failure resistance.

Abstract

Optimizing ceramic/metal multilayer coatings requires understanding how repeated interfaces influence microstructural evolution and mechanical failure. In this study, TiN/Rh multilayer coatings with different bilayer repetition numbers (n = 1, 3, 6, 10, and 15) were deposited on commercially pure titanium substrates by magnetron sputtering while maintaining constant cumulative nominal deposition times of 60 min for TiN and 15 min for Rh. Their crystalline structure, surface morphology, coating thickness, and scratch failure behavior were systematically investigated. Increasing the repetition number resulted in broader Rh (111) and TiN (200) diffraction reflections and a reduction in coating thickness from approximately 475 to 356 nm. The lateral Rh surface feature size decreased from 61.6 nm at n = 1 to a minimum of 43.8 nm at n = 10. The highest mean values of Lc1 and Lc2 were obtained at n = 3, reaching 47.7 ± 2.7 and 63.4 ± 2.1 N, respectively, before decreasing substantially to 9.5 ± 1.2 and 15.2 ± 1.2 N at n = 15. These findings demonstrate that increasing the number of ceramic/metal interfaces does not necessarily improve scratch failure resistance. Instead, multilayer architecture and its accompanying structural and thickness variations must be considered together when optimizing TiN/Rh coatings.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers