Salt-Supported Thermal Annealing of Polylactic Acid Components Produced by Fused Deposition Modeling: Effects on Tensile and Impact Properties
Sebastian Gnapowski, Ernest Gnapowski, Jacek Czerwiński, Karol Bożek, Katarzyna Rafał
Key points
From the paper's conclusion- Polylactic acid (PLA) components produced by fused deposition modeling (FDM) often exhibit anisotropic mechanical behavior associated with their layer-by-layer architecture.
Abstract
Polylactic acid (PLA) components produced by fused deposition modeling (FDM) often exhibit anisotropic mechanical behavior associated with their layer-by-layer architecture. Specimens were embedded in mechanically ground and manually compacted food-grade sodium chloride. The specimens were produced using a Creality K2 Pro printer with a direct-drive extruder and black PLA filament supplied by Plast-Spaw. The oven was preheated to 115 °C, and the holding interval of at least 160 min began when the monitored temperature in the salt bed reached 100 ± 5 °C. Five specimens per experimental group are included in the reported mechanical datasets, subject to the outcome-specific exclusions described in the Methods. For vertically printed specimens, the reported mean tensile strengths before and after treatment were 30.05 and 30.01 MPa, respectively, while the corresponding mean elongations were 8.88% and 8.29%. For horizontally printed specimens, the mean tensile strengths were 53.31 and 54.93 MPa, and the mean elongations were 10.21% and 10.13%, respectively. Charpy pendulum impact testing was performed in 2025. The impact-test specimens had a V-shaped notch with a nominal depth of 2 mm and a notch-root radius of 0.25 mm, in accordance with the geometry specified in ISO 179-1. The reported normalized impact results increased from 5.23 ± 0.55 to 6.74 ± 1.06 kJ/m2 for the vertical orientation and from 5.30 ± 0.51 to 17.19 ± 3.26 kJ/m2 for the horizontal orientation. FTIR spectra from one untreated specimen and one annealed specimen retained the characteristic absorption pattern of PLA, although several peak positions shifted. The horizontal-annealed elongation mean (10.13%) was calculated from four valid measurements, whereas the corresponding tensile-strength mean was calculated from five maximum-force results.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Post-Print Annealing of FDM-Printed Polylactic Acid: Mapping Strength, Crystallinity, and α′/α Polymorph Composition via a Replicated Taguchi L9 DesignPolymers · 2026
- Vacuum and Non-Vacuum Hydrothermal Annealing as a Post-Processing of MEX PLA on Tensile Response and Fracture Characteristics.Polymers · 2026
- Experimental analysis and optimization of the influence of layer height, infill pattern, and nozzle temperature on tensile strength, hardness, and relative density of FDM-PLA printsInternational Polymer Processing · 2026
- Effect of Annealing on the Mechanical Properties of Carbon Fiber-Reinforced PLA.Polymers · 2026
- Definitive screening design coupled with entropy‐weighted grey relational analysis for optimizing wear and strength of FDM PLAPolymer International · 2026
- Effect of post-printing annealing on the tensile behavior of stainless-steel wire mesh–reinforced PLA composites fabricated using material extrusionAdvances in Mechanical Engineering · 2026