Experimental Study on a Novel Early-Age High-Strength Shield Muck-Based Synchronous Grouting Material
Chun Li, Liyuan Yu, Zunbin Gao, Fuao Liu, Wei Li, Mengyang Yan, Hao Lu, Zhihao Dai,
Key points
From the paper's conclusion- The results indicate that the shield muck investigated in this study has potential for reuse in synchronous grouting materials.
Abstract
Large quantities of shield muck generated during urban shield tunnelling require sustainable disposal routes, yet synchronous grouting materials incorporating high contents of shield muck often suffer from insufficient early strength or poor stability. In this study, shield muck from the Jinan Metro was dried, ground, and sieved to obtain particles smaller than 1 mm, and subsequently used as a major solid constituent, together with fly ash and mineral powder, to prepare a muck-based synchronous grouting material. A conventional grout incorporating river sand as the aggregate was selected as a reference for evaluating strength development. A total of 72 mix-proportion tests were conducted to systematically investigate the effects of the water-to-solid ratio (w/s; 0.25, 0.275, 0.30, and 0.325), mineral powder replacement ratio for cement (0 and 50%), fly ash content (10%, 15%, and 20% by mass of total solid), and shield muck content (65%, 70%, and 75% by mass of total solid) on grout consistency, bleeding rate, setting time, consolidation shrinkage ratio, compressive strength, and flexural strength. The results showed that the water-to-solid ratio was a key factor governing grout consistency, bleeding behavior, and strength development. For the investigated muck source and pretreatment, the preferred mixture was selected at a water-to-solid ratio of 0.275, with 50% of the cement replaced by mineral powder, a fly ash content of 10%, and a shield muck content of 70%. This mix exhibited a consistency of 130.7 mm, bleeding rate of 1.77%, consolidation shrinkage ratio of 2.69%, initial and final setting times of 625 min (10.42 h) and 1160 min (19.33 h), respectively. The compressive strengths at 3, 7, and 28 d reached 1.76, 3.29, and 9.70 MPa, respectively, and the 28 d flexural strength was 3.08 MPa. Compared with conventional grouting materials incorporating river sand as the aggregate, the proposed material exhibited rapid early-age strength development and substantially improved mechanical performance. The results indicate that the shield muck investigated in this study has potential for reuse in synchronous grouting materials. Further research could investigate the net environmental benefits and potential economic benefits associated with the reuse of waste shield muck.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Performance Optimization of Shield Muck-Based Grouting Materials Using Rice Husk Ash and Micro-Expansive Agents.Materials (Basel, Switzerland) · 2026
- Optimisation of Simultaneous Grouting and Analysis of Lining Structural Response in Shield Tunnels Crossing Rivers Under Complex Geological ConditionsAdvances in Civil Engineering · 2026
- Mix proportion optimization and strength prediction of regenerated filling materials based on an SVR data-driven methodJournal of Physics: Conference Series · 2026
- Degradation of Mechanical Properties and Micro-Scale Damage Mechanisms of Mudstone-Type Soft Rock Under Hydro-Mechanical Coupling: A Case Study of the Baoshishan Tunnel, Western YunnanGeotechnics · 2026
- Optimization of anti-dispersion grouting material parameters for leakage treatment of tunnels in water-rich sandy cobble stratumCase Studies in Construction Materials · 2026
- Sustainable alkali‐activated grouting material incorporating industrial solid wastes for ground and structural strengtheningStructural Concrete · 2026