Materials

Study on the Interfacial Microstructure and Corrosion Behavior of TA2–Q345 Explosively Welded Joint in Marine Environments

Zhen Zhang, Chenhui Hu, Xin Huang, Shuhua Lu, Jing Li, Lin Liu

Key points

From the paper's conclusion
  • This study characterized the microstructure and corrosion behavior of the TA2–Q345 joint (Joint) in 3.5 wt.% NaCl solution and compared it with the TA2 cladding (CM) and the Q345 substrate (SM) at an exposed area of 1 cm2, with a Ti/steel area ratio of 1:4 for the Joint.

Abstract

TA2–Q345 explosively welded composite plates combine the corrosion resistance of titanium with the strength and cost-effectiveness of steel for marine applications. Once the joint cross-section is exposed, the heterogeneous bonding interface becomes a critical yet underexamined corrosion site. This study characterized the microstructure and corrosion behavior of the TA2–Q345 joint (Joint) in 3.5 wt.% NaCl solution and compared it with the TA2 cladding (CM) and the Q345 substrate (SM) at an exposed area of 1 cm2, with a Ti/steel area ratio of 1:4 for the Joint. The interface showed a periodic wavy morphology with vortex zones containing pores and dark inclusions. EDS revealed elemental mixing across the interface, while XRD identified FeTi and Fe2Ti intermetallic compounds (IMCs), with XPS providing supporting evidence of Fe–Ti bonding. The interfacial microhardness peak is attributed mainly to these IMCs, with grain refinement and strain hardening as possible contributions. Polarization and electrochemical impedance spectroscopy measurements indicated a corrosion-resistance ranking of CM > Joint > SM, consistent with the overall trend in apparent weight loss. Within the exposed joint, corrosion occurred preferentially on the steel side, a pattern consistent with possible galvanic interaction between titanium and steel. Iron oxides and hydroxides were identified among the corrosion products, including FeO(OH), Fe(OH)3, and Fe3O4. These findings highlight the susceptibility of the steel region to corrosion when the joint cross-section is exposed to chloride-containing environments.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers