Materials

Alkali-Activated Mortars from Municipal Solid Waste Incineration Bottom Ash: Optimisation of NaOH Molarity and Curing Temperature by Response Surface Methodology

Katarzyna Kalinowska-Wichrowska, Krzysztof Granatyr, Marta Kosior-Kazberuk, Adam Masłoń, Jurgita Malaiškienė, Karolina Baluta, Julia Skorbiłowicz

Key points

From the paper's conclusion
  • The results show that MSWI BA has promising mechanical potential for non-structural cement-free mortars, subject to environmental and durability assessments.

Abstract

Municipal solid waste incineration bottom ash (MSWI BA) is an abundant mineral residue whose valorisation as a precursor for alkali-activated binders supports circular-economy objectives. This study investigates cement-free alkali-activated mortars prepared with ground MSWI BA (8/16 mm fraction), CEN standard sand and sodium hydroxide (NaOH) solution. A central composite design (CCD) with two factors—curing temperature (45–105 °C) and NaOH molarity (4–12 M, at a constant activator-solution mass)—and ten series (four factorial, four axial and two centre points) was used to model the 28-day flexural strength, compressive strength and water absorption. The MSWI BA was characterised by X-ray fluorescence (XRF), X-ray diffraction (XRD), scanning electron microscopy (SEM), laser granulometry and the Chapelle pozzolanic-activity test. The ground ash (mean particle size ≈8 µm, Blaine specific surface area 491 m2/kg, Chapelle pozzolanic activity 547 mg Ca(OH)2/g) consisted mainly of quartz and anorthite with a pronounced amorphous phase. The highest 28-day compressive strength (22.9 MPa) and flexural strength (5.50 MPa) were measured at 60 °C and 6 M NaOH, whereas the lowest water absorption (7.89%) was obtained at 75 °C and 4 M NaOH; excessive molarity (12 M) and temperature extremes (45 and 105 °C) deteriorated the hardened matrix. Second-order response surface models fitted to the ten batch means (R2 = 0.81–0.93) located a model-based optimum near 70–75 °C and 5–6 M NaOH; with the batch as the experimental unit, however, the model was statistically significant only for flexural strength (F(5,4) = 10.03, p = 0.022). Three independent confirmation batches prepared at 72.5 °C and 5.5 M NaOH reproduced the predicted properties closely (measured 21.7 MPa compressive strength, 5.3 MPa flexural strength and 7.6% water absorption versus predicted 21.9 MPa, 5.2 MPa and 8.0%), validating the model-based optimum. The results show that MSWI BA has promising mechanical potential for non-structural cement-free mortars, subject to environmental and durability assessments.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers