Experimental Characterization and Finite Element Thermomechanical Analysis of the AlSi16Cu3MgNiCrMn Piston Alloy

Boyan Dochev, Atanasi Tashev, Desislava Dimova, Karel Trojan, Veselin Tsonev, Nikola Kuzmanov, Georgi Avdeev, Ivan Zahariev

Key points

From the paper's conclusion
  • To complement the experimental investigation, a three-dimensional finite element model of a piston–ring–cylinder liner assembly was developed to evaluate the thermomechanical response under representative engine operating conditions.

Abstract

A new, non-standardized, complex-alloyed hypereutectic aluminium–silicon alloy, AlSi16Cu3MgNiCrMn, has been developed for the manufacture of internal combustion engine pistons. The alloy was subjected to modification treatments using sodium (Na) and phosphorus (P), followed by solution treatment, water quenching, and artificial aging (T6). Its microstructure, phase composition, and mechanical properties were investigated using optical metallography, X-ray diffraction (XRD), hardness measurements, and tensile testing at room and elevated temperatures. Following heat treatment, the primary silicon crystals exhibited an average size of approximately 23.9 μm, while the eutectic silicon particles underwent partial fragmentation and spheroidization, with their average dimensions decreasing from approximately 11.0 to 8.2 μm. XRD analysis identified Si, Al3.96Si0.04, Al4Cu9, and Al57Mn12 phases. At room temperature (25 °C), the alloy exhibited a hardness of 109 HB, an ultimate tensile strength of 257 MPa, and an elongation at break of 0.7%. Tensile strength decreased with increasing temperature, reaching 223 MPa at 150 °C, 173 MPa at 250 °C, and 83 MPa at 350 °C. To complement the experimental investigation, a three-dimensional finite element model of a piston–ring–cylinder liner assembly was developed to evaluate the thermomechanical response under representative engine operating conditions. Sequentially coupled thermal and structural analyses were performed, incorporating temperature-dependent material properties, combustion gas pressure, lateral piston forces, and contact interactions. The calculated maximum equivalent von Mises stresses were approximately 127 and 113 MPa for the two investigated loading conditions, with corresponding minimum factors of safety of approximately 1.4 and 1.5. The combined experimental and numerical results demonstrate the potential of the investigated alloy for piston applications and provide a basis for further evaluation of its structural performance under elevated thermal and mechanical loads.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers