Materials (Basel, Switzerland)

The Effect of Waste Glass Fine Aggregate and Waste Glass Powder on the Sulfate Resistance and Microstructure of Recycled Mortar.

Hao Ren, Ling Luo, Yongjun Qin, Jilong Liu

College of Civil Engineering and Architecture, Xinjiang University, Urumqi 830017, China.

Key points

From the paper's conclusion
  • These findings support the potential use of waste glass in recycled mortar exposed to sulfate-rich environments.

Abstract

To improve the sulfate resistance of recycled mortar, waste glass fine aggregate (WGFA) and waste glass powder (GP) were used to partially replace recycled fine aggregate and cement, respectively. Sulfate wet-dry cycling tests were conducted on the mortar specimens using a 5% Na2SO4 solution. Sulfate resistance was assessed using mass loss rates and compressive corrosion resistance coefficients, while microstructural changes were examined by scanning electron microscopy with energy-dispersive X-ray spectroscopy (SEM-EDS), thermogravimetric analysis (TGA), and mercury intrusion porosimetry (MIP). Among the four mixtures, S20P15 (20% WGFA and 15% GP) exhibited the best sulfate resistance after 120 cycles, with a mass loss rate of 3.8% and a compressive corrosion resistance coefficient 13.3% higher than that of the control. MIP and SEM observations showed that S20P15 had relatively lower total porosity and fewer visible cracks, consistent with its improved durability. TGA revealed differences in thermal decomposition characteristics among the mixtures. The observed performance may be related to changes in aggregate grading, pore structure, and hydration-related characteristics associated with the combined incorporation of WGFA and GP. These findings support the potential use of waste glass in recycled mortar exposed to sulfate-rich environments.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers