Effect of Shielding Gas Purity on Microstructure and Strain-Rate-Dependent Tensile Behavior of GTAW CP-Ti Welds.
Ana B Salazar-Zapata, Victor H Baltazar-Hernandez, Enrique A Lopez-Baltazar, Francisco Alvarado-Hernandez, Daolun L Chen
UAZ-Quantum Laboratory, Department of Manufacturing and Materials Science & Engineering, Universidad Autonoma de Zacatecas, Zacatecas 98000, Mexico. · Department of Mechanical, Industrial, and Mechatronics Engineering, Toronto Metropolitan University, Toronto, ON M5B 2K3, Canada.
Key points
From the paper's conclusion- This study investigated the influence of shielding gas purity on the microstructure and strain-rate-dependent tensile behavior of gas-tungsten-arc-welded commercially pure titanium Grade 2 joints.
Abstract
This study investigated the influence of shielding gas purity on the microstructure and strain-rate-dependent tensile behavior of gas-tungsten-arc-welded commercially pure titanium Grade 2 joints. Two argon grades were compared: ultra-high-purity (UHP, 99.999%) and high-purity (HP, 99.997%). UHP shielding achieved full penetration at ~9.5% lower heat input, producing a narrower welded region. Welding transformed the fine, weakly textured base metal into coarser, moderately textured heat-affected zones and strongly textured lamellar/acicular fusion zones. HP shielding produced higher fusion-zone hardness, potentially associated with interstitial strengthening. All tensile specimens fractured within the heat-affected zone, while UHP shielding resulted in higher strength, elongation, and strain-rate sensitivity. Welding altered both the magnitude and strain evolution of strain-rate sensitivity, consistent with the combined influence of grain structure, crystallographic texture, and deformation mechanisms involving slip and twinning.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Effect of Oxygen Contents in Shielding Gas on GTAW Joints of Commercially Pure TitaniumMetals · 2026
- Effect of Welding Speed on the Properties of Laser Beam Welded 3 mm Thick Ti-6Al-4V Butt JointsAdvances in Materials Science · 2026
- Study on microstructure and properties of titanium alloy wall fabricated by laser-TIG arc.PloS one · 2026
- Low-temperature bonding of W90 tungsten heavy alloy using Sn-2Al filler metal by ultrasonic-assisted coating technologyTransactions of Nonferrous Metals Society of China · 2026
- Continuous and pulsed TIG welded joint of ASTM A105-AISI 316L steels: Characterization of microstructure, mechanical properties, and fracture analysisJournal of Materials Research and Technology · 2025
- The Characters of Second Phases and Texture of Aluminum Alloy Thin-Walled Capsule Welded Joints at Typical HIP Temperature.Materials (Basel, Switzerland) · 2026