Structure-Property Tailoring of Long-Chain PDMS-Based Polyurethanes for Flexible MXene Strain Sensors.
Marija V Pergal, Ivana O Mladenović, Ivan Pešić, Aleksa Bakoč, Zdravko Džambaski, Milena Rašljić Rafajilović, Darko Micić, Dana Vasiljević-Radović,
Institute of Chemistry, Technology and Metallurgy, University of Belgrade, National Institute of the Republic of Serbia, Njegoševa 12, 11000 Belgrade, Serbia. · Faculty of Physical Chemistry, University of Belgrade, Studentski trg 12-16, 11000 Belgrade, Serbia.
Key points
From the paper's conclusion- The MXene/PU-50 sensor exhibited a gauge factor of 65.9 over 0–8% strain, response/recovery times of 138/58 ms, and a signal-to-noise ratio (SNR) of 39.5 dB, demonstrating a reversible piezoresistive response with good short-term repeatability and the feasibility of using a long-chain PDMS-based PU substrate for rapid and sensitive wearable strain sensing.
Abstract
Flexible and mechanically adaptable polymer substrates are critical for conformable wearable sensors capable of accurately tracking human motion and vital parameters. Here, crosslinked polyurethanes (PUs) were synthesized from a long-chain poly(ethylene oxide)-b-poly(dimethylsiloxane)-b-poly(ethylene oxide) (PEO-PDMS-PEO) macrodiol (Mn = 2400 g mol-1), 4,4'-methylenediphenyl diisocyanate, and a multifunctional hyperbranched polyester, with soft-segment contents of 15-70 wt.%. Mechanical, structural, surface, and thermal properties were evaluated by indentation methods (nanoindentation, microindentation, and microindentation creep), XRD, AFM, wettability measurements, TGA, and DSC. Increasing the soft-segment content markedly reduced stiffness; Young's modulus decreased from 1713 MPa to 112 MPa to 80 MPa as the soft segment content was increased from 30 wt.% to 50 wt.% to 70 wt.%, respectively, while hardness decreased from 89 to 4 MPa. The predominantly amorphous networks retained good thermal stability, with degradation temperature (T(10%)) values of 249-291 °C and glass transition temperature (Tg) values of 21-25 °C. Increasing the soft-segment content also increased surface roughness (Rq: 18.3-250 nm) and water contact angle (approximately 45-90°), indicating progressive surface enrichment by the low-surface-energy PDMS-containing phase. PU-50 was selected as the finger-motion sensor substrate and coated with Ti3C2Tx MXene by spray deposition. The MXene/PU-50 sensor exhibited a gauge factor of 65.9 over 0-8% strain, response/recovery times of 138/58 ms, and a signal-to-noise ratio (SNR) of 39.5 dB, demonstrating a reversible piezoresistive response with good short-term repeatability and the feasibility of using a long-chain PDMS-based PU substrate for rapid and sensitive wearable strain sensing.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Embedding‐Depth‐Controlled MXene/PDMS Strain Sensors for Biocompatible Human Joint Motion MonitoringInternational Journal of Energy Research · 2026
- Flexible MXene/PDMS/SWCNT nanocomposites for high-performance resistive strain sensors with potential application in low temperatureJournal of Materials Science Composites · 2026
- High-Performance PDMS Elastomers Constructed via Oxalyl Dihydrazide for Thermoreversible Bonding in Flexible Electronics.ACS applied materials & interfaces · 2026
- Construct a visible thermochromic multi-mode sensor based on MXene-deposited grating-striped PDMSJournal of Physics: Conference Series · 2026
- Skin-Inspired Piezoresistive Sensor Based on Hierarchical Structures and Lignocellulosic Bioplastic Electrodes with Ultrahigh SensitivityACS Applied Materials & Interfaces · 2025
- Molecular Steric Engineering Enables High-Strength and Self-Healing Polyurethane Elastomer for Flexible and Sensitive NanosensorsACS Applied Polymer Materials · 2026