Two-Stage Sulfuric Acid Leaching of Vanadium-Bearing Carbonaceous Siliceous Ore: Oxidative Pressure Leaching, Kinetics, and Mechanism.
Dosmurat Aitkulov, Anar Mukhametzhanova, Akmaral Rakhym, Aliya Margulanovna Alimzhanova
Republican State Enterprise National Center for Complex Processing of Mineral Raw Materials of the Republic of Kazakhstan, Zhandosov st., 67, Almaty 050036, Kazakhstan. · Department of Physical Chemistry, Catalysis and Petrochemistry, Faculty of Chemistry and Chemical Technology, Farabi University, Al-Farabi ave., 71, Almaty 050040, Kazakhstan.
Key points
From the paper's conclusion- The combined results indicate selective acid–oxidative dissolution of accessible vanadium-bearing phases followed by increasingly restricted extraction from resistant mineral domains within the silica-rich residual matrix.
Abstract
Efficient vanadium recovery from carbonaceous siliceous ores is challenging because of the complex mineral occurrence of vanadium and the high chemical resistance of the quartz-rich matrix. In this study, a two-stage processing scheme comprising atmospheric decarbonization-neutralization followed by oxidative autoclave leaching was developed for vanadium-bearing quartzite from the Balasausqandiq deposit (Kyzylorda Region, Kazakhstan). Under the optimized autoclave conditions (140 °C, 120 min, 150 kg t-1 H2SO4, 5 kg t-1 HNO3, 3 atm O2, and a solid-to-liquid ratio of 1:1), 88.4% of vanadium was extracted. XRD and SEM-EDS analyses revealed preferential dissolution of reactive V- and Fe-bearing minor phases, while the quartz-rich matrix remained largely preserved, producing a residue containing 72.5 wt.% SiO2 and <0.01 wt.% carbon. Among the shrinking-core models tested, the product-layer diffusion model provided the closest fit to the available kinetic data (R2 = 0.9787-0.9865). A three-temperature Arrhenius analysis over 120-140 °C yielded a preliminary apparent activation energy of 54.55 kJ mol-1. Thermodynamic calculations supported the oxidative pathway, showing that V(IV) oxidation by O2 is favorable at 140 °C (∆rG° = -75.1 kJ mol-1). The combined results indicate selective acid-oxidative dissolution of accessible vanadium-bearing phases followed by increasingly restricted extraction from resistant mineral domains within the silica-rich residual matrix. The proposed process integrates efficient vanadium recovery with the generation of a silica-rich residue with potential for use as a secondary metallurgical feedstock, subject to further evaluation.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Selective two-stage redox-controlled acidic leaching and alkaline hydrothermal leaching of vanadium and tungsten from spent selective catalytic reduction catalysts with experimental and thermodynamic evaluationSeparation and Purification Technology · 2026
- Endogenous calcification-assisted mineral-phase activation enhances Acidithiobacillus ferrooxidans-mediated vanadium bioleaching from vanadium-titanium blast furnace slagFrontiers in Microbiology · 2026
- Vanadium, Titanium, and Iron Extraction from Titanomagnetite Ore by Salt Roasting and 21st-Century SolventsSeparations · 2025
- Synergistic depassivation of ZVI intensifies persulfate activation for high-efficiency vanadium leaching in a sono‑Fenton‑like systemUltrasonics Sonochemistry · 2026
- Microwave-Assisted Sulfuric Acid Leaching of Vanadium from Pre-Decalcified Vanadium-Bearing Steel Slag.Molecules (Basel, Switzerland) · 2026
- Mechanism of Mechanical Activation-Assisted Selective Decalcification of Vanadium-Bearing Steel Slag.Molecules (Basel, Switzerland) · 2026