Feasibility and Performance Evaluation of Asphalt Concrete Cores for Rockfill Dams.

Chawakorn Rewtragulpaibul, Saravut Jaritngam, Tanawan Wannawong, Peerawat Puengpapat

Royal Irrigation Department, Ministry of Agriculture and Cooperatives, Bangkok 10300, Thailand. · Faculty of Engineering, Prince of Songkla University, Songkhla 90110, Thailand.

Key points

From the paper's conclusion
  • Relative to the conventional clay-core baseline, a 0.50-m-thick asphalt concrete core with shell slopes of 1 V:1.5 H and 1 V:1.4 H reduced the calculated embankment volume per unit dam length by 21.11% and 24.83%, respectively, with corresponding global factors of safety of 1.655 and 1.557.

Abstract

This study investigated the potential use of asphalt concrete produced with locally sourced limestone and granite aggregates as an impervious core material in rockfill dams. An independent laboratory program evaluated 16 mixture conditions comprising two aggregate types, asphalt cement contents of 6% and 7%, and nominal target air-void contents of 1-4%. Marshall, hydraulic-conductivity, and consolidated-undrained triaxial tests were conducted to characterize the mixtures. The reported hydraulic conductivity ranged from 2.9549 × 10-10 to 3.8887 × 10-5 cm/s, while effective cohesion and friction angle ranged from 165.7 to 540.3 kPa and 34.07° to 55.61°, respectively. Four core-property datasets corresponding to a 2% target air-void content were evaluated using two-dimensional GeoStudio analyses under steady-state and rapid-drawdown conditions. Steady-state seepage discharge ranged from 1.967 × 10-9 to 6.7191 × 10-6 m3/s, with downstream global factors of safety of 2.209-2.215. The upstream global factor of safety at Day 7 of rapid drawdown was 2.041 for all four datasets. The granite mixture containing 7% asphalt cement and a target air-void content of 2% (Granite AC7% AV2%) was subsequently selected as a representative, rather than optimal, core-property dataset for a separate steady-state geometry comparison. Relative to the conventional clay-core baseline, a 0.50-m-thick asphalt concrete core with shell slopes of 1 V:1.5 H and 1 V:1.4 H reduced the calculated embankment volume per unit dam length by 21.11% and 24.83%, respectively, with corresponding global factors of safety of 1.655 and 1.557. A supplementary rapid-drawdown assessment of the steepest alternative yielded an upstream global factor of safety of 1.473 at Day 6, the lowest among the reported daily results. The findings provide comparative laboratory data and case-specific numerical results for preliminary assessment of asphalt concrete dam cores. Hydraulic acceptance and field-scale suitability are not established, and further experimental verification and numerical sensitivity assessments remain necessary before application.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers

Feasibility and Performance Evaluation of Asphalt Concrete Cores for Rockfill Dams — Science Skim