From the paper's conclusion- To characterize curing heat release and temperature evolution during interface damage repair in China Railway Track System (CRTS) II slab ballastless track, the curing kinetics and thermal properties of repair slurry for interface damage (RSID) were investigated.
Abstract
To characterize curing heat release and temperature evolution during interface damage repair in China Railway Track System (CRTS) II slab ballastless track, the curing kinetics and thermal properties of repair slurry for interface damage (RSID) were investigated. Non-isothermal differential scanning calorimetry (DSC) was conducted at four heating rates, and the apparent activation energy was determined using the Kissinger, Ozawa, and Starink methods. An n-order curing kinetic model and a two-parameter (m, n) autocatalytic curing kinetic model were established and compared. The specific heat capacity and thermal conductivity were determined using laser flash analysis (LFA), and corresponding temperature-dependent constitutive models were established. These material properties were incorporated into a three-dimensional transient heat transfer finite element model considering curing heat release, which was validated through curing temperature-rise experiments. The results show that the curing exothermic peak shifts toward higher temperatures with increasing heating rate. The average apparent activation energy obtained from the three methods is 55.21 kJ/mol. The two-parameter autocatalytic model provides better agreement with the experimental curing-rate curves than the n-order model, with R2 values exceeding 0.960. The specific heat capacity increases approximately linearly with temperature, whereas the thermal conductivity exhibits an exponential growth trend. The simulated and measured temperature histories agree closely, with an R2 value of 0.979, a peak temperature difference of 0.2 °C, and a difference of 3 s in the time to reach the peak. The simulated temperature field shows greater heat accumulation in the interior, with higher temperatures internally and lower temperatures near the boundaries. These findings provide material parameters and a thermal analysis basis for optimizing interface damage grouting repair processes in ballastless track and support subsequent analyses of thermal deformation and the development of measures to control secondary damage during repair.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Calculation model for the thermal conductivity of concrete considering microstructural characteristicsCase Studies in Thermal Engineering · 2026
- Development of a Cracking Resistance Index for Ballastless Track Slab Concrete: Evaluation and Mixture Optimization.Materials (Basel, Switzerland) · 2026
- A temperature-indexed concrete damage plasticity framework for thermomechanical analysis of concrete structuresJournal of Engineering and Applied Science · 2025
- Early-Age Thermo-Mechanical Response of a Concrete Spine-Beam Bridge During Construction: Local Heat Accumulation and Restrained CoolingApplied Sciences · 2026
- Full-process temperature control and crack prevention of roller compacted concrete in water conservancy projectsFrontiers in Mechanical Engineering · 2026
- Crack Extension Characteristics of Continuously Reinforced Concrete and Asphalt Composite Pavements Under Thermo-Mechanical Coupling and Non-Uniform Tire LoadingCoatings · 2026