Microstructural Evolution and Compressive Strength Degradation of Hydraulic Asphalt Concrete Under Extreme Freeze-Thaw Cycles.
Xubin Huang, Zhe Miao, Guangshan Shi, Yongzhi Liu, Shengting Wang, Shuangchao Lei, Xiangyang Li, Jiansheng Wang
State Key Laboratory of Cryospheric Science and Frozen Soil Engineering, Northwest Institute of Eco-Environment and Resources, Chinese Academy of Sciences, Lanzhou 730000, China. · Power China Northwest Engineering Corporation Limited, Xi'an 710100, China.
Key points
From the paper's conclusion- The results show that compressive strength gradually decreased with increasing freeze–thaw cycles, while mercury-accessible pore volume, relative mass change, and interfacial defects progressively increased.
Abstract
Driven by China's carbon peaking and carbon neutrality goals, pumped-storage hydropower projects have developed rapidly, while power stations in Northwest China face challenges posed by extreme temperature conditions. Unlike previous studies on asphalt mixtures under conventional freeze-thaw conditions, this study employs multiscale characterization methods to investigate the deterioration behavior of dense-graded hydraulic asphalt concrete under extreme temperature cycling. SBS-modified asphalt concrete specimens were vacuum-saturated and subjected to 0, 5, 10, 15, and 20 accelerated freeze-thaw cycles over a temperature range from -45 to + 60 °C. Uniaxial compression tests, relative mass change measurements, MIP, CT with three-dimensional pore reconstruction, and SEM were employed. The results show that compressive strength gradually decreased with increasing freeze-thaw cycles, while mercury-accessible pore volume, relative mass change, and interfacial defects progressively increased. After 20 cycles, compressive strength decreased by 9.29%, while the mercury-accessible volume of large capillary pores increased by 19.05%. SEM observations of the selected fields revealed more pronounced pores and cracks near the aggregate-asphalt mastic interface. These findings suggest that the aggregate-asphalt mastic interface is one of the relatively vulnerable regions under extreme cyclic exposure, although changes in the asphalt binder itself may also contribute to material deterioration. This study provides experimental evidence for understanding the deterioration behavior of hydraulic asphalt concrete under extreme temperature conditions.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Fatigue Performance and Pore Characteristics of SBS/Micro Carbon Fiber Composite-Modified Asphalt Concrete for Ultra-Thin Overlays.Polymers · 2026
- Effects of Early Surface‐Layer Environmental Degradation on Structural Response and Fatigue Risk of Asphalt Pavements in Cold RegionsAdvances in Civil Engineering · 2026
- Experimental study on dynamic mechanical properties and damage mechanisms models of concrete under freeze-thaw cyclesScientific Reports · 2026
- Freeze-Thaw-Induced Deterioration and Failure Mechanisms of Permeable Concrete in Cold Regions.Materials (Basel, Switzerland) · 2026
- Freeze–Thaw Durability and Meso-Scale Damage Mechanism of Concrete Incorporating Granulated Blast-Furnace Slag as Fine AggregateBuildings · 2026
- Damage Evolution and Mechanical Deterioration of Concrete Incorporating Waste-Derived Artificial Aggregates Under Freeze–Thaw CyclesSustainability · 2026