Burr Detection and Edge Condition in Ceramic Brushing of Glass and Carbon Fabric-Reinforced Composites Using Recurrence Analysis of Force Signals: A Feasibility Study.
Jakub Matuszak, Krzysztof Ciecieląg
Department of Production Engineering, Mechanical Engineering Faculty, Lublin University of Technology, Nadbystrzycka 36, 20-618 Lublin, Poland.
Key points
From the paper's conclusion- On one edge of glass (GFRP) and carbon (CFRP) fabric-reinforced specimens, positioned at 45° to the tool axis, chamfered segments 0.1–0.4 mm deep, representing a burr-free edge, alternated with as-milled segments with burrs.
Abstract
Burrs formed during the machining of fibre-reinforced polymer composites reduce safety and product quality and are usually inspected off-process. This study assessed whether as-milled edge segments with burrs can be distinguished from burr-free chamfered segments on the basis of the force signal recorded during edge brushing, as a first step towards in-process burr detection, and how brush fibre stiffness affects the edge condition. On one edge of glass (GFRP) and carbon (CFRP) fabric-reinforced specimens, positioned at 45° to the tool axis, chamfered segments 0.1-0.4 mm deep, representing a burr-free edge, alternated with as-milled segments with burrs. The edges were brushed with four ceramic-fibre brushes of increasing stiffness (S1-S4) at constant parameters, and the force signal was analysed using recurrence plots (RP) and recurrence quantification analysis (RQA). Chamfers 0.1 mm deep did not produce unambiguous changes in the recurrence structure. For the stiff brushes (S3, S4), chamfers 0.2-0.4 mm deep produced local RP densifications consistent with their location. In the RQA, for chamfers ≥ 0.2 mm, DET (determinism) and L (average diagonal line length) mostly rose above and LAM(laminarity) and TT (trapping time) fell below the burred-edge reference levels. The chamfer width produced by brushing increased with fibre stiffness, from 588 to 1040 µm (GFRP) and from 389 to 1005 µm (CFRP). Under the tested conditions, the force signal distinguished the two edge conditions; its use for detecting burrs themselves requires further validation on edges with quantified burrs.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Assessment and Selection of Ceramic Brush Stiffness and Orientation Angle for Edge Finishing of Milled GFRP and CFRP Composites Using Recurrence AnalysisMaterials · 2026
- Monitoring of tool wear in CFRP drilling based on acoustic emissionJournal of Polymer Engineering · 2026
- Finite element modeling of cutting forces and surface integrity in milling of GFRP and CFRP composites with acoustic emission monitoringScientific Reports · 2026
- Experimental optimization of abrasive brush deburring for burr control in automotive manufacturingResults in Materials · 2026
- Effects of CFRP chip particle size on surface chemical activity during high-speed cutting: underlying mechanisms.RSC advances · 2026
- A comprehensive dynamic force model involved in grinding of B₄ C ceramicsInternational Journal of Extreme Manufacturing · 2026