Effect of Nb Content on Tribocorrosion Behavior of TiZrNbTa Refractory Multi-Principal Element Alloys in Sodium Chloride Solution.
Zening Wang, Yi Zhang, Jinping Wu, Yu Yan, Lijie Qiao
Beijing Advanced Innovation Center for Materials Genome Engineering, Corrosion and Protection Center, Institute for Advanced Materials and Technology, University of Science and Technology Beijing, Beijing 100083, China.
Key points
From the paper's conclusion- In this work, the effect of Nb content on the microstructure, passive film stability, and tribocorrosion behavior of TiZrNbTa refractory multi-principal element alloys (RMPEAs) was evaluated in 0.9 wt.% NaCl solution.
Abstract
In this work, the effect of Nb content on the microstructure, passive film stability, and tribocorrosion behavior of TiZrNbTa refractory multi-principal element alloys (RMPEAs) was evaluated in 0.9 wt.% NaCl solution. Three designed alloys, Ti45Zr45Nb5Ta5, Ti35Zr35Nb25Ta5 and Ti31.67Zr31.67Nb31.67Ta5, were examined via electrochemical measurements, reciprocating sliding tests, X-ray photoelectron spectroscopy and surface/subsurface characterization. All alloys exhibited a single-phase body-centered cubic (BCC) solid solution. Increasing Nb refined dendritic grains but aggravated elemental segregation and reduced hardness from 320 ± 10 HV to 230 ± 10 HV. Reductions in corrosion and passive current densities demonstrated improved corrosion resistance and passive film stability. However, repassivation kinetics deteriorated because reduced Ti and Zr availability limited their preferential oxidation, which governed rapid passive film formation on fresh surfaces. Accordingly, higher Nb did not yield superior tribocorrosion resistance. The wear mechanism shifted from mild abrasive wear with continuous tribofilms toward severe ploughing, plastic deformation, delamination and microcracking. Under open-circuit potential (OCP) conditions, the average friction coefficient increased from 0.51 ± 0.05 to 0.78 ± 0.08, and the tribocorrosion rate rose from (3.75 ± 0.11) × 10-3 to (10.27 ± 0.30) × 10-3 mm3·N-1·m-1. Pure mechanical wear accounted for 70.72-79.11% of total material loss, and corrosion-accelerated wear dominated the synergistic component. The degraded performance at high Nb contents arose from the combined influence of decreased hardness, severe segregation, pit-triggered crack growth and suppressed surface work hardening. All of these factors amplified corrosion-accelerated wear. These findings revealed the dual function of Nb in TiZrNbTa RMPEAs. Nb stabilized the passive film while exacerbating tribocorrosion damage.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Role of Niobium and Tantalum on the Diffusivity of Point Defects in the Passive Film of TiZrNbTa Multi-Principal Element Alloys in Sodium Chloride Solution.Materials (Basel, Switzerland) · 2026
- Tribology of TiNbCr MPEA: Insights into tribolayer formation and resulting wear resistanceJournal of Materials Research · 2026
- Tribo-corrosion behavior of novel beta alloy Ti–25Nb–4Ta–8Sn in contact with various tipsKoroze a ochrana materiálu · 2026
- Laves phase tailored heterostructures for excellent tribocorrosion resistance in a laser cladding Ti-based composite coatingJournal of Materials Research and Technology · 2026
- High‐Strength and Ductile TiNbZrTa BCC MPEA With Heterogeneous Microstructure for Orthopedic ImplantsAdvanced Healthcare Materials · 2026
- In Situ Crystalline‐Amorphous Composite Oxide Structure Suppressing Thermal Wear Instability for Refractory Multi‐Principal Element AlloyAdvanced Functional Materials · 2026